| 100 parts resin to 9.5 parts hardener. TIGA R-915 is a medium viscosity versatile epoxy bonding system that exhibits unusually high thermal conductivity and low thermal expansion. It is recommended for electronic/electrical bonding and encapsulating applications that require a unique combination of excellent wetting, flow, good thermal expansion coefficients, thermal shock resistance, high heat transfer capabilities and outstanding electrical properties. Fully cured TIGA R-915 is highly resistant to weather, water, gases and vapors, petroleum lubricants and fuels and many mild acids and alkalis. Information provided by Resin Technology Group. |