MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Morgan Advanced Ceramics RBSN Reaction bonded silicon nitride Mac-RBSNS
Categories: Ceramic; Nitride

Material Notes: An advanced synthetic ceramic with a nominal Si3N4 content of 99%. Reaction bonded silicon nitride (RSBN) is made by directly reacting compacted silicon powder with nitrogen to produce porous components of relatively low density and possessing exceptional thermal.

Prime Features:

  • Porous, low density material
  • Exceptional resistance to thermal downshock
  • Excellent resistance to wetting and attack by molten non-ferrous alloys containing aluminum, magnesium, copper, zinc and lead.
  • Low thermal conductivity
  • Good electrical resistance
Typical Applications:
  • Welding jigs and fixtures
  • Molten non-ferrous metal handling systems
  • Riser tubes and transfer tubes
  • Delivery systems and degassing systems
  • Special crucibles
Production Capabilities:
  • Net shape forming
  • Prototype, batch and volume production

Information provided by Morgan Advanced Materials

Key Words: RBSN
Vendors:
Available Properties
  • Density, fired
  • Open Porosity, nominal, apparent
  • Modulus of Elasticity, Young's
  • Flexural Strength, 3 point
  • Compressive Strength
  • Volume Resistivity
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air, no load
  • Si3N4
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.