MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics RBSN Reaction bonded silicon nitride Mac-RBSNS
Categories: Ceramic; Nitride

Material Notes: An advanced synthetic ceramic with a nominal Si3N4 content of 99%. Reaction bonded silicon nitride (RSBN) is made by directly reacting compacted silicon powder with nitrogen to produce porous components of relatively low density and possessing exceptional thermal.

Prime Features:

  • Porous, low density material
  • Exceptional resistance to thermal downshock
  • Excellent resistance to wetting and attack by molten non-ferrous alloys containing aluminum, magnesium, copper, zinc and lead.
  • Low thermal conductivity
  • Good electrical resistance
Typical Applications:
  • Welding jigs and fixtures
  • Molten non-ferrous metal handling systems
  • Riser tubes and transfer tubes
  • Delivery systems and degassing systems
  • Special crucibles
Production Capabilities:
  • Net shape forming
  • Prototype, batch and volume production

Information provided by Morgan Advanced Materials

Key Words: RBSN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.50 g/ccfired
Open Porosity 20 %nominal, apparent
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 170 GPa
@Temperature 20.0 °C
Young's
Flexural Strength 200 MPa
@Temperature 20.0 °C
3 point
Compressive Strength 650 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+10 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.10 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 1.10 J/g-°C
Thermal Conductivity 12.0 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 1300 °Cno load
 
Component Elements PropertiesOriginal ValueComments
Si3N4 99 %
 
Descriptive Properties
Colorgray
Thermal Downshock>600 sC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Techical Ceramics Ekasic® S Silicon Nitride
Goodfellow High Thermal Conductivity Silicon Nitride
3M Techical Ceramics Ekatherm® Silicon Nitride
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB
Goodfellow Gas Pressure Sintered Silicon Nitride Si3N4

CMORF5083 / 200321

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.