MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Suqian Unitechem Light Stabilizer 944
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: Poly-{[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidyl)imino]-1,6-hexanediyl[(2,2,6,6-tetramethyl-4-piperidyl)imino]}

CAS NO.: 70624-18-9

Molecular Formula: [C35H64N8]n

High molecular light stabilizer with multiple functional groups. It can be used in low density PE film, PP tape, EVA film, ABS, PP fiber, PPE, polyacetals, polyamides, polyurethanes, PVC, PVC blending material, polystyrene, rubber and viscose. It can work with UV absorbent because its special structure and large molecular weight. It can also be used in film and fiber, and as an antioxidant and heat stabilizer of polymer. The dosage of agricultural film is 2%.

Soluble in organic solvents, slightly soluble in methanol, and insoluble in water.

Information Provided by Suqian Unitechem Co., Ltd.

Vendors:
Available Properties
  • Bulk Density
  • Density, Relative density
  • Volatiles
  • Molecular Weight
  • Ash
  • Softening Point
  • Transmission, Visible, 425nm
  • Transmission, Visible, 450nm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.