MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Suqian Unitechem Light Stabilizer 944
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: Poly-{[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidyl)imino]-1,6-hexanediyl[(2,2,6,6-tetramethyl-4-piperidyl)imino]}

CAS NO.: 70624-18-9

Molecular Formula: [C35H64N8]n

High molecular light stabilizer with multiple functional groups. It can be used in low density PE film, PP tape, EVA film, ABS, PP fiber, PPE, polyacetals, polyamides, polyurethanes, PVC, PVC blending material, polystyrene, rubber and viscose. It can work with UV absorbent because its special structure and large molecular weight. It can also be used in film and fiber, and as an antioxidant and heat stabilizer of polymer. The dosage of agricultural film is 2%.

Soluble in organic solvents, slightly soluble in methanol, and insoluble in water.

Information Provided by Suqian Unitechem Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.548 - 0.646 g/cc
Density 1.01 g/cc
@Temperature 20.0 °C
Relative density
Volatiles <= 1.0 %
Molecular Weight 2100 - 3000 g/mol
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Softening Point 110 - 130 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 93 %425nm
 >= 95 %450nm
 
Descriptive Properties
AppearanceWhite powder or granule
Weight Loss Temperature (°C)> 270

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics PVC-ELS Polyvinylchloride, Electrically Conductive Grade
Overview of materials for PVC, Rigid Grade
Overview of materials for PVC, Molded

PSUQI01 / 103984

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.