MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
G-3 Fiberglass Phenolic Laminate Sheet
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths.

Physical strength, resiliency, ease and versatility of fabrication, and excellent electrical properties make phenolic laminates useful as support components in a wide range of mechanical and electrical applications. Phenolic laminates are strong, stiff, and have high impact and compressive strengths. They do not soften upon re-heating, so they are easy to saw, drill, tap, and machine with ordinary tools. Glass-based grades have the highest dimensional stability and mechanical strength, as well as low moisture absorption. However, they are not as easily machined as paper or cotton fabric laminates.

Information provide by Boedeker Plastics.

Key Words: G3 Fiber Reinforced Composite
Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570, 24 hrs.
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength at Break, ASTM D638, Crosswise
  • Tensile Strength at Break, ASTM D638, Lengthwise
  • Flexural Strength, ASTM D790, Crosswise
  • Flexural Strength, ASTM D790, Lengthwise
  • Flexural Modulus, ASTM D790, Crosswise
  • Flexural Modulus, ASTM D790, Lengthwise
  • Compressive Strength, ASTM D695
  • Izod Impact, Notched, ASTM D256, Crosswise
  • Izod Impact, Notched, ASTM D256, Lengthwise
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, Short Time; 1/8 inch
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • CTE, linear, ASTM D696, Lengthwise
  • CTE, linear, Transverse to Flow, ASTM D696, Crosswise
  • Thermal Conductivity, ASTM C177
  • Maximum Service Temperature, Air
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.