MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
G-3 Fiberglass Phenolic Laminate Sheet
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths.

Physical strength, resiliency, ease and versatility of fabrication, and excellent electrical properties make phenolic laminates useful as support components in a wide range of mechanical and electrical applications. Phenolic laminates are strong, stiff, and have high impact and compressive strengths. They do not soften upon re-heating, so they are easy to saw, drill, tap, and machine with ordinary tools. Glass-based grades have the highest dimensional stability and mechanical strength, as well as low moisture absorption. However, they are not as easily machined as paper or cotton fabric laminates.

Information provide by Boedeker Plastics.

Key Words: G3 Fiber Reinforced Composite
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccASTM D792
Water Absorption 2.65 %24 hrs.; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 110ASTM D785
Tensile Strength at Break 34000 psiCrosswise; ASTM D638
 42000 psiLengthwise; ASTM D638
Flexural Strength 34000 psiCrosswise; ASTM D790
 40500 psiLengthwise; ASTM D790
Flexural Modulus 1400 ksiCrosswise; ASTM D790
 1800 ksiLengthwise; ASTM D790
Compressive Strength 55000 psiASTM D695
Izod Impact, Notched 11.0 ft-lb/inCrosswise; ASTM D256
 12.0 ft-lb/inLengthwise; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 7.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 460 V/milShort Time; 1/8 inch; ASTM D149
Dissipation Factor 0.023
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.30 µin/in-°F
@Temperature 20.0 °C
Lengthwise; ASTM D696
CTE, linear, Transverse to Flow 18.0 µm/m-°C
@Temperature 20.0 °C
Crosswise; ASTM D696
Thermal Conductivity 2.00 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 170 °C
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LE Phenolic Laminate
Phenolic 30%, Graphite fabric 70%
Ensinger Tecapeek® Polyetheretherketone (PEEK)
G-10 Fiberglass Epoxy Laminate Sheet
Overview of materials for Phenolic, Novolac, Cellulose Filled

PGLAM00 / 41885

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.