MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Phenolic, Novolac, Cellulose Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Cellulose Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 - 1.60 g/cc0.0379 - 0.0578 lb/in³Average value: 1.34 g/cc Grade Count:29
Water Absorption 0.0800 - 1.90 %0.0800 - 1.90 %Average value: 0.822 % Grade Count:11
Linear Mold Shrinkage 0.00200 - 0.00400 cm/cm0.00200 - 0.00400 in/inAverage value: 0.00294 cm/cm Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 70.0 - 11570.0 - 115Average value: 89.9 Grade Count:8
Tensile Strength, Ultimate 38.0 - 120 MPa5510 - 17400 psiAverage value: 64.1 MPa Grade Count:20
Flexural Yield Strength 55.0 - 175 MPa7980 - 25400 psiAverage value: 92.8 MPa Grade Count:28
Flexural Modulus 4.80 - 14.0 GPa696 - 2030 ksiAverage value: 7.84 GPa Grade Count:19
Compressive Yield Strength 70.0 - 350 MPa10200 - 50800 psiAverage value: 185 MPa Grade Count:28
Shear Strength 10.0 - 20.0 MPa1450 - 2900 psiAverage value: 15.0 MPa Grade Count:8
Izod Impact, Notched 0.315 - 0.683 J/cm0.590 - 1.28 ft-lb/inAverage value: 0.512 J/cm Grade Count:10
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 100000 - 1.00e+10 ohm100000 - 1.00e+10 ohmAverage value: 9.46e+8 ohm Grade Count:14
Dielectric Constant 5.50 - 6.005.50 - 6.00Average value: 5.67 Grade Count:6
Dielectric Strength 1.00 - 14.6 kV/mm25.4 - 371 kV/inAverage value: 6.99 kV/mm Grade Count:10
Dielectric Breakdown >= 20000 V
@Temperature 90.0 - 90.0 °C
>= 20000 V
@Temperature 194 - 194 °F
Average value: 23300 V Grade Count:6
 >= 10000 V
@Temperature 90.0 - 90.0 °C
>= 10000 V
@Temperature 194 - 194 °F
Average value: 23300 V Grade Count:8
 >= 10000 V
@Time 20.0 - 60.0 sec
>= 10000 V
@Time 0.00556 - 0.0167 hour
Average value: 23300 V Grade Count:8
Dissipation Factor 0.0500 - 0.05500.0500 - 0.0550Average value: 0.0517 Grade Count:6
Arc Resistance 60.0 - 150 sec60.0 - 150 secAverage value: 101 sec Grade Count:8
Comparative Tracking Index 100 V100 VAverage value: 100 V Grade Count:8
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 - 47.0 µm/m-°C10.0 - 26.1 µin/in-°FAverage value: 32.1 µm/m-°C Grade Count:7
CTE, linear, Transverse to Flow 52.0 - 69.0 µm/m-°C28.9 - 38.3 µin/in-°FAverage value: 58.0 µm/m-°C Grade Count:3
Thermal Conductivity 0.410 - 0.580 W/m-K2.85 - 4.03 BTU-in/hr-ft²-°FAverage value: 0.522 W/m-K Grade Count:4
Maximum Service Temperature, Air 150 °C302 °FAverage value: 150 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 165 - 282 °C329 - 540 °FAverage value: 201 °C Grade Count:11
Flammability, UL94 HB - V-0HB - V-0Grade Count:9
 
Processing PropertiesMetricEnglishComments
Mold Temperature 150 - 180 °C302 - 356 °FAverage value: 166 °C Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac
G-3 Fiberglass Phenolic Laminate Sheet
Overview of materials for Phenolic, Novolac, Glass Filled
LE Phenolic Laminate

O2736 / 78099

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.