MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Hiflex CA 7700 A Thermoplastic Elastomeric Olefin
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hiflex CA 7700 A is a reactor soft thermoplastic polyolefin (rTPO) , manufactured using the Lyondell Basell proprietary Catalloy process technology and is stabilized with a standard additive package. The grade is available in natural colored pellet form. Hiflex CA 7700 A is designed for use in injection molding or extrusion compounds when good processability, optimum mechanical and good dimensional stability, are key properties. Thanks to its tailored elastomeric phase, Hiflex CA 7700 A features high softness and high toughness at very low temperature and provide high thermal characteristics. Hiflex CA 7700 A is used as a blending partner to improve the overall performances of durable and technical compounds. Hiflex CA 7700 A is highly compatible with a wide range of polyolefins and soft plastics. This grade can be either blended or co-extruded with other materials to provide the required property balance

Status: Developmental

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Automotive Parts; Impact Modification; Wire & Cable

Market: Automotive; Compounding; Electrical / Electronics; Industrial, Building & Construction; Wire & Cable

Processing Method: Compounding; Extrusion Flat-die; Injection Molding

Attribute: Good Electrical Properties; Good Processability; Haptics; High Filler Loading Capability; Low Melting Temperature; Low Shrinkage; Low Temperature Impact Resistance; Scratch Resistant

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Density, ISO 1183-1, Method A
  • Melt Flow, ISO 1133-1
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, ISO 527-1, -2
  • Tensile Strength, Yield, ISO 527-1, -2
  • Elongation at Break, ISO 527-1, -2
  • Elongation at Yield, ISO 527-1, -2
  • Flexural Modulus, ISO 178
  • Charpy Impact, Notched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Melting Point, ISO 11357-3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75B-1, -2, Unannealed
  • Vicat Softening Point, ISO 306, A50
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell LYB (former Equistar)

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.