MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAKEEP® 4000 CFL30 PEEK, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: VESTAKEEP® 4000 CFL30 is a carbon fiber reinforced polyether ether ketone for injection molding. The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 CFL30 are characterized by low flammability. VESTAKEEP® 4000 CFL30 can be processed by common injection molding machines for thermoplastics. The manufacturer recommends a melt temperature between 380°C and 400°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C. VESTAKEEP® 4000 CFL30 is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Pigmentation may affect values.
Dry properties listed below
Industrial Sector: Energy, Oil and Gas
Processing: Injection molding
Additives: Carbon fiber
Applications: Encapsulation

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ISO 1133
  • Hardness, Shore D, ASTM D2240, annealed
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, ISO 527
  • Elongation at Break, ISO 527, annealed
  • Elongation at Break, ISO 527
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ASTM D638, annealed
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Charpy Impact, Notched, ISO 179/1eA
  • Melt Temperature, Injection Molding
  • Mold Temperature, Injection Molding
  • Injection Velocity, Injection Molding
  • Moisture Content, ISO 15512
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.