MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® 4000 CFL30 PEEK, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: VESTAKEEP® 4000 CFL30 is a carbon fiber reinforced polyether ether ketone for injection molding. The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 CFL30 are characterized by low flammability. VESTAKEEP® 4000 CFL30 can be processed by common injection molding machines for thermoplastics. The manufacturer recommends a melt temperature between 380°C and 400°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C. VESTAKEEP® 4000 CFL30 is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Pigmentation may affect values.
Dry properties listed below
Industrial Sector: Energy, Oil and Gas
Processing: Injection molding
Additives: Carbon fiber
Applications: Encapsulation

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Melt Flow 24.0 g/10 min
@Load 21.6 kg,
Temperature 400 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 92.0
@Time 1.00 sec
annealed; ASTM D2240
Tensile Strength at Break 0.265 MPaASTM D638
 245 MPaISO 527
Tensile Strength 245 MPaISO 527
Elongation at Break 2.00 %annealed; ISO 527
 2.00 %ISO 527
Tensile Modulus 24000 MPaISO 527
 24161.6 MPaannealed; ASTM D638
Flexural Strength 400 MPaASTM D790
Flexural Modulus 2120 MPaASTM D790
Charpy Impact, Notched 11.0 kJ/m²ISO 179/1eA
 
Processing PropertiesOriginal ValueComments
Melt Temperature 420 °CInjection Molding
Mold Temperature 200 °CInjection Molding
Injection Velocity 200 mm/secInjection Molding
Moisture Content 0.150 %ISO 15512
Shelf Life 24.0 Month
@Temperature 30.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7835 / 324967

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.