MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Park Aerospace Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.

Key Features and Benefits:

  • Controlled flow for ease of processing
  • Self adhesive for honeycomb or foam sandwich laminates without the use of film adhesive
  • Flexible cure temperature 180°F to 250°F
  • Good electrical properties
  • Flame and fire retardant per FAR 25.853
  • Wet service temperatures up to 160°F

Applications/Qualifications:

  • Radomes
  • Aircraft Interiors
  • Secondary Aircraft Structures
  • Sandwich Panels
  • MRI Resonators
  • Widely specified on commercial and military aircraft programs

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors:
Available Properties
  • Volatiles, 8 min
  • Thickness, Per Ply
  • Tensile Strength, Yield, Flatwise (sandwich); Bag Surface
  • Tensile Strength, Yield, Flatwise (sandwich); Mold Surface
  • Tensile Strength, Yield, ASTM D638, 0° Direction, Dry
  • Tensile Strength, Yield, ASTM D638, 0° Direction, Wet
  • Tensile Strength, Yield, ASTM D638, 0° Direction, Wet
  • Tensile Strength, Yield, ASTM D638, 0° Direction, Dry
  • Tensile Strength, Yield, ASTM D638, 0° Direction, Dry
  • Tensile Strength, Yield, ASTM D638, 0° Direction, Dry
  • Tensile Modulus, ASTM D638, 0° Direction, Wet
  • Tensile Modulus, ASTM D638, 0° Direction, Wet
  • Tensile Modulus, ASTM D638, 0° Direction, Dry
  • Tensile Modulus, ASTM D638, 0° Direction, Dry
  • Tensile Modulus, ASTM D638, 0° Direction, Dry
  • Tensile Modulus, ASTM D638, 0° Direction, Dry
  • Flexural Strength, ASTM D790, Wet
  • Flexural Strength, ASTM D790, Dry
  • Flexural Strength, ASTM D790, Dry
  • Flexural Strength, ASTM D790, Wet
  • Flexural Strength, ASTM D790, Dry
  • Flexural Strength, ASTM D790, Dry
  • Flexural Modulus, ASTM D790, Wet
  • Flexural Modulus, ASTM D790, Dry
  • Flexural Modulus, ASTM D790, Dry
  • Flexural Modulus, ASTM D790, Wet
  • Flexural Modulus, ASTM D790, Dry
  • Flexural Modulus, ASTM D790, Dry
  • Compressive Strength, ASTM D695, Wet
  • Compressive Strength, ASTM D695, Dry
  • Compressive Strength, ASTM D695, Dry
  • Compressive Strength, ASTM D695, Wet
  • Compressive Strength, ASTM D695, Dry
  • Compressive Strength, ASTM D695, Dry
  • Compressive Modulus, ASTM D695, Wet
  • Compressive Modulus, ASTM D695, Dry
  • Compressive Modulus, ASTM D695, Dry
  • Compressive Modulus, ASTM D695, Wet
  • Compressive Modulus, ASTM D695, Dry
  • Compressive Modulus, ASTM D695, Dry
  • Shear Strength, ASTM D2344, Short-Beam, Dry
  • Shear Strength, ASTM D2344, Short-Beam, Wet
  • Shear Strength, ASTM D2344, Short-Beam, Dry
  • Shear Strength, ASTM D2344, Short-Beam, Wet
  • Shear Strength, ASTM D2344, Short-Beam, Dry
  • Shear Strength, ASTM D2344, Short-Beam, Dry
  • Dielectric Constant
  • Dielectric Constant
  • Dissipation Factor
  • Dissipation Factor
  • Glass Transition Temp, Tg, Dry; DMA
  • Gel Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Park Aerospace, former Park Electrochemical Corp.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.