MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.

Key Features and Benefits:

  • Controlled flow for ease of processing
  • Self adhesive for honeycomb or foam sandwich laminates without the use of film adhesive
  • Flexible cure temperature 180°F to 250°F
  • Good electrical properties
  • Flame and fire retardant per FAR 25.853
  • Wet service temperatures up to 160°F

Applications/Qualifications:

  • Radomes
  • Aircraft Interiors
  • Secondary Aircraft Structures
  • Sandwich Panels
  • MRI Resonators
  • Widely specified on commercial and military aircraft programs

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.5 %
@Temperature 135 °C
8 min
Thickness 9.00 milPer Ply
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 549 - 693 psiFlatwise (sandwich); Bag Surface
 840 psiFlatwise (sandwich); Mold Surface
 47000 psi
@Temperature 93.3 °C
0° Direction, Dry; ASTM D638
 52000 psi
@Temperature 71.1 °C
0° Direction, Wet; ASTM D638
 59000 psi
@Temperature 21.1 °C
0° Direction, Wet; ASTM D638
 65000 psi
@Temperature 71.1 °C
0° Direction, Dry; ASTM D638
 72000 psi
@Temperature 21.1 °C
0° Direction, Dry; ASTM D638
 95000 psi
@Temperature -53.9 °C
0° Direction, Dry; ASTM D638
Tensile Modulus 3300 ksi
@Temperature 71.1 °C
0° Direction, Wet; ASTM D638
 3400 ksi
@Temperature 21.1 °C
0° Direction, Wet; ASTM D638
 3500 ksi
@Temperature -53.9 °C
0° Direction, Dry; ASTM D638
 3700 ksi
@Temperature 21.1 °C
0° Direction, Dry; ASTM D638
 3700 ksi
@Temperature 71.1 °C
0° Direction, Dry; ASTM D638
 3900 ksi
@Temperature 93.3 °C
0° Direction, Dry; ASTM D638
Flexural Strength 65.0 ksi
@Temperature 71.1 °C
Wet; ASTM D790
 66.0 ksi
@Temperature 93.3 °C
Dry; ASTM D790
 77.0 ksi
@Temperature 71.1 °C
Dry; ASTM D790
 80.0 ksi
@Temperature 21.1 °C
Wet; ASTM D790
 95.0 ksi
@Temperature 21.1 °C
Dry; ASTM D790
 117 ksi
@Temperature -53.9 °C
Dry; ASTM D790
Flexural Modulus 2700 ksi
@Temperature 71.1 °C
Wet; ASTM D790
 2800 ksi
@Temperature 93.3 °C
Dry; ASTM D790
 2900 ksi
@Temperature 71.1 °C
Dry; ASTM D790
 3000 ksi
@Temperature 21.1 °C
Wet; ASTM D790
 3200 ksi
@Temperature -53.9 °C
Dry; ASTM D790
 3200 ksi
@Temperature 21.1 °C
Dry; ASTM D790
Compressive Strength 47.0 ksi
@Temperature 71.1 °C
Wet; ASTM D695
 52.0 ksi
@Temperature 93.3 °C
Dry; ASTM D695
 55.0 ksi
@Temperature 71.1 °C
Dry; ASTM D695
 56.0 ksi
@Temperature 21.1 °C
Wet; ASTM D695
 66.0 ksi
@Temperature 21.1 °C
Dry; ASTM D695
 84.0 ksi
@Temperature -53.9 °C
Dry; ASTM D695
Compressive Modulus 3500 ksi
@Temperature 71.1 °C
Wet; ASTM D695
 3500 ksi
@Temperature 71.1 °C
Dry; ASTM D695
 3500 ksi
@Temperature 93.3 °C
Dry; ASTM D695
 3600 ksi
@Temperature 21.1 °C
Wet; ASTM D695
 3600 ksi
@Temperature 21.1 °C
Dry; ASTM D695
 3700 ksi
@Temperature -53.9 °C
Dry; ASTM D695
Shear Strength 5.20 ksi
@Temperature 93.3 °C
Short-Beam, Dry; ASTM D2344
 6.00 ksi
@Temperature 71.1 °C
Short-Beam, Wet; ASTM D2344
 6.50 ksi
@Temperature 71.1 °C
Short-Beam, Dry; ASTM D2344
 8.00 ksi
@Temperature 21.1 °C
Short-Beam, Wet; ASTM D2344
 9.00 ksi
@Temperature 21.1 °C
Short-Beam, Dry; ASTM D2344
 11.5 ksi
@Temperature -53.9 °C
Short-Beam, Dry; ASTM D2344
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.2
@Frequency 9.375e+9 Hz
 4.2
@Frequency 1.80e+10 Hz
Dissipation Factor 0.013
@Frequency 9.375e+9 Hz
 0.013
@Frequency 1.80e+10 Hz
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 115 °CDry; DMA
 
Processing PropertiesOriginal ValueComments
Gel Time 4.00 min
Shelf Life 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Climbing Drum Peel (in-lb/3in)14.7ASTM D1781; Mold Surface, 75°F
 14.8ASTM D1781; Bag Surface, 75°F
Fabric Area Weight (g/m²)303.5
Long Beam Flexure (P/Y lb/in)152 / 124Bag Surface
 201Mold Surface
Long Beam Flexure Strength (lbs)157 / 130Bag Surface
 205Mold Surface
Prepreg Resin Content (%)39
Resin Flow (%)14275°F, 50psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Park Aerospace Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced
Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric
Solvay CYCOM® 985 Epoxy + Glass Fabric Laminate
Park Aerospace Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Park Aerospace Nelcote® E-722 Epoxy Prepreg, 7781 E-Glass Reinforced

PPARK019 / 89291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.