MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
General Plastics LAST-A-FOAM® FR-4515 High Density, Rigid Foam
Categories: Other Engineering Material

Material Notes: Product Description: LAST-A-FOAM® high-density, rigid foam products are cost-effective, versatile, strong and durable. They are manufactured using our unique chemical formulas to be exceptionally uniform and consistent in all physical properties. The FR-4500 is a grain-free, machineable tooling board for styling and design models, master models, masters for composite and layup tools, and for mold and foundry patterns. The material also serves as an excellent wood alternative for outdoor signage and display manufacturing. Available in densities from 10 to 50 lbs. per cubic foot.

Key Performance Benefits:

  • Special formulation creates shavings when material is machined, causing less dust
  • Excellent consistency and uniformity throughout entire mass of material
  • Dimensional stability
  • No warp or bow in sheets
  • Large sheets (up to 48” x 96”), thick sheets (up to 22”) available
  • Custom sizes available
Applications:
  • Design prototypes
  • Appearance or “sight” models
  • Styling models
  • Architectural models
  • Master models
  • Temporary models
  • Trim, jigs, and fixtures
  • Thermoforming tools
  • Prototype foundry patterns
  • Mold patterns
  • Topographical maps
  • Dimensional check-fixtures
  • Molds for low-temperature casting (<200 ºF)
  • Prototype/low-volume Vacuum-forming tools
  • CAD model proofs/NC program proofs
  • Tooling aids
  • Molds for low-temperature curing prepregs (<200 ºF)

Information provided by General Plastics Manufacturing Company

Vendors:
Available Properties
  • Density, ASTM D1622
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D1623, Parallel to Rise
  • Tensile Strength, ASTM D1623, Perpendicular to Rise
  • Tensile Strength, ASTM D1623
  • Flexural Strength, ASTM D790 Method 1-A, Rise Parallel to Beam Thick.
  • Flexural Strength, ASTM D790 Method 1-A, Rise Parallel to Test Span
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ASTM D790 Method 1-A, Rise Parallel to Beam Thick.
  • Flexural Modulus, ASTM D790 Method 1-A, Rise Parallel to Test Span
  • Compressive Strength, ASTM D1621
  • Compressive Strength, ASTM D1621, Perpendicular to Rise
  • Compressive Strength, ASTM D1621, Parallel to Rise
  • Compressive Strength, ASTM D1621, Perpendicular to Rise
  • Compressive Strength, ASTM D1621, Parallel to Rise
  • Compressive Modulus, ASTM D1621
  • Compressive Modulus, ASTM D1621, Perpendicular to Rise
  • Compressive Modulus, ASTM D1621, Parallel to Rise
  • Compressive Modulus, ASTM D1621, Perpendicular to Rise
  • Compressive Modulus, ASTM D1621, Parallel to Rise
  • Poissons Ratio
  • Shear Modulus, ASTM C273
  • Shear Strength, ASTM C273
  • CTE, linear, GP Method
  • Thermal Conductivity, ASTM C518
  • Glass Transition Temp, Tg, ASTM E1545-05
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.