MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials AquaStik® 2901 Latex  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: AquaStik® 2901 contains a high modulus, fast crystallizing polychloroprene homopolymer made in an anionic colloidal system.

Main Feature: This latex is resistant to low temperature exposure, and gives adhesives with very fast strength development.

Suggested End Uses:

  • Adhesives for bonding foam to various substrates
  • Foam adhesives
  • Fabric saturants

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccLatex at 25°C
Density 1.23 g/ccPolymer
Particle Size 0.13 µmAverage
pH 12.525°C
Brookfield Viscosity >= 6.00e+7 cP
@Temperature 25.0 °C
6 rpm or 30 rpm
Surface Tension 37.6 dynes/cm
 
Descriptive Properties
Electrolyte StabilityFairly Good
Emulsifying AgentPotassium salt of resin acid
Freeze/thawResistant to -5°C
Mechanical StabilityGood
Polymer TypeFast Crystallizing Homopolymer
Solids56-60 wt%
StorageGood

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitriflex Nitrilatex L-2108 Styrene Butadiene Latex
Master Bond LTX 119 Pressure Sensitive Acrylic Adhesive Latex Compound
Abatron AboSeal 8104-17 Acrylic-Latex Based Sealant and Caulk; High-Density
Mallard Creek Polymers Rovene® 6023 Carboxylated Acrylic Copolymer Latex
Abatron AboSeal 8104-9 Polysulfide, Thixotropic or Self-Leveling Sealant and Caulk

PDVE17 / 34059

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.