MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mallard Creek Polymers Rovene® 6023 Carboxylated Acrylic Copolymer Latex
Categories: Polymer

Material Notes: Applications: Rovene® 6023 in portland cement mixtures results in increased adhesion to most substrates, improved water resistance, increased flexural strength and good resistance to UV light. Rovene® 6023 does not contain antifoam. The addition of an effective antifoam is generally required to avoid a high air content in the hydraulic cementitious mixture. Many antifoam products have been found effective at levels of 2.5% wet on wet by mass. Rovene® 6023 is suggested as a polymer modifier for hydraulic cementitious mixtures for repair, basecoats for EIFS, decorative overlays and tile grouts or mortars requiring low odor during application. Addition of 5 - 15% (d/d Portland cement) improves flexibility, strength and water resistance.

Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6023 Material Safety Data Sheet before handling, storing, or using this product.

Information provided by Mallard Creek Polymers

Key Words: portland cement
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 46 - 48 %46 - 48 %
pH 8.5 - 108.5 - 10
Brookfield Viscosity <= 400 cP<= 400 cP#20/200 rpm
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 12.0 °C53.6 °F
 
Descriptive Properties
EmulsifiersAnionic
Minimum Film Formation Temperature (°C)16

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials AquaStik® 2901 Latex
Master Bond LTX 119 Pressure Sensitive Acrylic Adhesive Latex Compound
Nitriflex Nitrilatex L-2108 Styrene Butadiene Latex
Michelman® Licomer® T 51 Acrylic copolymer dispersion
Unifrax Fiberfrax® Topcoat™ 3000 Coating Cement

PMCP006 / 104663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.