MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco HDAX® SAE 40 Ashless Gas Engine Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron HDAX Ashless Gas Engine Oils are superior quality, ashless, gas engine oils.

They are formulated with ISOSYN™ base stocks and a carefully balanced ashless package of dispersant, antioxidant, extreme pressure, and corrosion inhibitor additives.

They are formulated without bright stock for all two-stroke and selected four-stroke high speed, high output, turbocharged, natural gas engines operating at full capacity.

Chevron HDAX Ashless Gas Engine Oils provide exceptionally clean engine parts, even under severe operating conditions and extended overhaul intervals. They effectively eliminate the formation of crankcase sludge and maintain clean intake and exhaust ports in two-stroke engines.

Chevron HDAX Ashless Gas Engine Oils eliminate serious problems encountered with ash-containing oils, such as spark plug fouling, pre-ignition, valve guttering, or burning. They reduce wear of piston rings and cylinder liners, and protect against corrosion of vital engine parts.

Applications

Chevron HDAX Gas Engine Oils are recommended for all two-cycle and selected four-cycle stationary engines that require a completely ashless-type engine oil and which use natural gas or synthetic natural gas as a fuel.

Chevron HDAX Gas Engine Oil SAE 30 has full Dresser-Rand (Ingersoll-Rand) approval for Category I, Naturally Aspirated Engines, and Category II, Low Level Turbo-charged engines. Chevron HDAX Gas Engine Oils are recommended for manufactured by Ajax, Caterpillar (except 3400, 3500 and 3600), Clark-Dresser, Cooper Bessemer (two-cycle), Dresser-Rand (Ingersoll-Rand) Categories I and II, Fairbanks-Morse/MEP, Waukesha VR and Intermediate/Clinton, and Worthington (four-cycle).

Key Words: CPS Number: 232307; MSDS Number: 7050
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 30.1 °30.1 °
Viscosity Measurement 9595Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 134 cSt134 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 13.5 cSt13.5 cStASTM D445
Ash 0.00 %0.00 %Sulfated Ash wt%
 
Chemical PropertiesMetricEnglishComments
Total Base Number 3.13.1ASTM D2896
 
Thermal PropertiesMetricEnglishComments
Pour Point -18.0 °C-0.400 °FASTM D97
Flash Point 260 °C500 °FASTM D92
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 0.067 %0.067 %
Zinc, Zn <= 0.0010 %<= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCHEV058 / 74673

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.