MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mytex Polymers AS78L-GM Polypropylene, Rubber modified, Compounded
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: AS78L-GM is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.

Key Applications: Bumper fascias, cladding and bodyside molding

Information provided by Mytex Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792
Melt Flow 25 g/10 minASTM D1238
Ash 7.0 %ASTM D5630
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ISO 868
Tensile Strength, Yield 16.0 MPa50 mm/min; ISO 527
Flexural Modulus 1060 MPaChord; 2 mm/min; ISO 178
Izod Impact, Notched (ISO) 50.0 kJ/m²
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °CISO 75-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® A 246M Nylon 66, Impact Grade, EH50
Celanese Zytel® ST801AHS NC010 PA66-HI
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating
Akro-Plastic Akromid® B3 S1 black (3726) PA 6 Conditioned, Cold Impact Resistant
AKG Polymers Vision PP PPC BL1008 Polypropylene Copolymer Compound

PMYTEX026 / 90316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.