MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the application, Borsoft SF203CF should be used preferably in blends with PP with high melt strength (HMS).

Borsoft SF203CF is specially suitable for sealing layer, textile back sheet, breathable compounds, and soft coating.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 230 °C
22 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133/DIN 5335
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 14.0 MPa2030 psiISO 527-2
Elongation at Yield 15 %15 %ISO 527-2
Tensile Modulus 0.450 GPa65.3 ksiISO 527-2
Flexural Modulus 0.400 GPa58.0 ksiDIN 53457/ISO 178
Charpy Impact, Notched 2.50 J/cm²11.9 ft-lb/in²ISO 179/1eA
 0.200 J/cm²
@Temperature -20.0 °C
0.952 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 35.0 °C95.0 °FISO 75 B
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C126 °FISO 75 A

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borpact™ SG930MO Polypropylene Copolymer
Borealis RJ370MO Polypropylene, Transparent Random Copolymer
Borealis Borsoft™ SG220MO Polypropylene Random Copolymer for Injection Molding
Celanese Celstran® PP-GF20-02 AF3001 Natural PP, 20% Glass Reinforced
Mytex Polymers AS78L-GM Polypropylene, Rubber modified, Compounded

PBOREA107 / 27414

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.