MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Latrobe Marvac 250 VIM-VAR ; 5 in. High Strength Maraging Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel; Maraging Steel

Material Notes: MARVAC 250 VIM-VAR is a low carbon maraging steel capable of 240,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which include a low rate of work hardening, good machinability and weldability, and a very simple heat treatment process. Marvac 250 is produced by vacuum induction melting followed by VAC-ARC remelting. This approach provides superior cleanness and a preferred ingot structure to enhance transverse mechanical properties. Marvac 250 is supplied in the solution annealed condition.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1840 MPa267000 psi
Tensile Strength, Yield 1725 - 1730 MPa
@Strain 0.2 %
250200 - 251000 psi
@Strain 0.2 %
Elongation at Break 12 - 12.2 %12 - 12.2 %
Reduction of Area 55 - 56 %55 - 56 %
Fracture Toughness >= 82.0 MPa-m½>= 74.6 ksi-in½
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.8 µm/m-°C
@Temperature 23.0 - 482 °C
6.00 µin/in-°F
@Temperature 73.4 - 900 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.10 %0.10 %
Carbon, C 0.010 %0.010 %
Cobalt, Co 7.75 %7.75 %
Iron, Fe 68.24 %68.24 %
Manganese, Mn 0.10 %0.10 %
Molybdenum, Mo 4.8 %4.8 %
Nickel, Ni 18.5 %18.5 %
Silicon, Si 0.10 %0.10 %
Titanium, Ti 0.40 %0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® VascoMax® C-250 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
ATI Allvac® VascoMax® C-300 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
AISI Grade 18Ni (200) Maraging Steel, Aged, 75 mm round bar, tested in longitudinal direction
AISI Grade 18Ni (250) Maraging Steel, Aged, 75 mm round bar, tested longitudinal
Latrobe Marvac 300 VIM-VAR ; 6.25 in. High Strength Maraging Steel

NTIMK047 / 19394

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.