System Message
Advertise with MatWeb!
Data sheets for over
185,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Material Category Search
User Input Problem
Find a Material Category:
Select a Material Category:
Carbon (866 matls)
Ceramic (10004 matls)
Fluid (7562 matls)
Metal (17052 matls)
Other Engineering Material (8063 matls)
Polymer (97635 matls)
Pure Element (507 matls)
Wood and Natural Products (398 matls)
Selected Material Category:
Search Results
There are
70
materials in the category
Maraging Steel
. If your material is not listed, please refer to our
search strategy
page for assistance in limiting your search.
Found
70
Results
-- Page
1
2
of
2
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Use Folder
Contains
New Folder Name
My Folder
Select
Material Name
1
Overview of materials for Maraging Steel
2
AISI Grade 18Ni (200) Maraging Steel, Annealed
3
AISI Grade 18Ni (200) Maraging Steel, Aged, 16 mm round bar, tested in longitudinal direction
4
AISI Grade 18Ni (200) Maraging Steel, Aged, 32 mm round bar, tested in longitudinal direction
5
AISI Grade 18Ni (200) Maraging Steel, Aged, 75 mm round bar, tested in longitudinal direction
6
AISI Grade 18Ni (200) Maraging Steel, Aged, 150 mm (2 in.) round bar, tested in longitudinal direction
7
AISI Grade 18Ni (200) Maraging Steel, Aged, 150 mm square bar, tested in transverse direction
8
AISI Grade 18Ni (200) Maraging Steel, Aged, 6 mm square bar, tested in transverse direction
9
AISI Grade 18Ni (200) Maraging Steel, solution annealed at 815°C (1500°F) for 1 hour, air cooled, aged at 480°C (900°F) for 3 hours
10
AISI Grade 18Ni (250) Maraging Steel, nominal annealed properties
11
AISI Grade 18Ni (250) Maraging Steel, Aged, 16 mm round bar, tested longitudinal
12
AISI Grade 18Ni (250) Maraging Steel, Aged, 32 mm round bar, tested longitudinal
13
AISI Grade 18Ni (250) Maraging Steel, Aged, 75 mm round bar, tested longitudinal
14
AISI Grade 18Ni (250) Maraging Steel, Aged, 150 mm square bar, tested longitudinal
15
AISI Grade 18Ni (250) Maraging Steel, Aged, 150 mm square bar, tested transverse
16
AISI Grade 18Ni (250) Maraging Steel, Aged, 6 mm sheet, tested transverse
17
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 455°C (850°F) for 3 hours
18
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 1 hour
19
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 3 hours
20
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 6 hours
21
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 510°C (950°F) for 3 hours
22
AISI Grade 18Ni (250) Maraging Steel, solution annealed at 815°C (1500°F) for 1 hour, air cooled, aged at 480°C (900°F) for 3 hours
23
AISI Grade 18Ni (300) Maraging Steel solution annealed at 815°C (1500°F) for 1 hour, air cooled, aged at 480°C (900°F) for 3 hours
24
AISI Grade 18Ni (300) Maraging Steel nominal annealed properties
25
AISI Grade 18Ni (300) Maraging Steel, Aged, round bar, tested longitudinal, 16 mm
26
AISI Grade 18Ni (300) Maraging Steel, Aged, round bar, tested longitudinal, 32 mm
27
AISI Grade 18Ni (300) Maraging Steel, Aged, round bar, tested longitudinal, 75 mm
28
AISI Grade 18Ni (300) Maraging Steel, Aged, square bar, tested longitudinal, 150 mm
29
AISI Grade 18Ni (300) Maraging Steel, Aged, square bar, tested transverse, 150 mm
30
AISI Grade 18Ni (300) Maraging Steel, Aged, sheet, tested transverse, 6 mm
31
AISI Grade 18Ni (300) Maraging Steel solution treated at 815°C (1500°F) for 15 minutes, air cooled, aged at 480°C (900°F) for 3 hours, 6.35 mm sheet
32
AISI Grade 18Ni (300) Maraging Steel solution treated at 815°C (1500°F) for 15 minutes, air cooled, aged at 480°C (900°F) for 3 hours, 3.18 mm sheet
33
AISI Grade 18Ni (300) Maraging Steel solution treated at 815°C (1500°F) for 15 minutes, air cooled, aged at 480°C (900°F) for 3 hours, 2.29 mm sheet
34
AISI Grade 18Ni (300) Maraging Steel solution treated at 815°C (1500°F) for 15 minutes, air cooled, aged at 480°C (900°F) for 3 hours, 1.65 mm sheet
35
AISI Grade 18Ni (300) Maraging Steel solution treated at 815°C (1500°F) for 15 minutes, air cooled, aged at 480°C (900°F) for 3 hours, 1.14 mm sheet
36
AISI Grade 18Ni (300) Maraging Steel solution treated at 815°C (1500°F) for 15 minutes, air cooled, aged at 480°C (900°F) for 3 hours, 0.64 mm sheet
37
AISI Grade 18Ni (300) Maraging Steel solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 455°C (850°F) for 3 hours, 3.18 mm sheet
38
AISI Grade 18Ni (300) Maraging Steel solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 1 hour, 3.18 mm sheet
39
AISI Grade 18Ni (300) Maraging Steel solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 3 hours, 3.18 mm sheet
40
AISI Grade 18Ni (300) Maraging Steel solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 6 hours, 3.18 mm sheet
41
AISI Grade 18Ni (300) Maraging Steel solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 510°C (950°F) for 3 hours, 3.18 mm sheet
42
AISI Grade 18Ni (350) Maraging Steel nominal annealed properties
43
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested longitudinal, round bar 16 mm
44
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested longitudinal, round bar 32 mm
45
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested longitudinal, round bar 75 mm
46
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested transverse, sheet 6 mm thick
47
AISI Grade 18Ni (350) Maraging Steel solution annealed at 815°C (1500°F) for 1 hour, air cooled, aged at 480°C (900°F) for 6 hours
48
1800 Maraging Steel
49
2000 Maraging Steel
50
2800 Maraging Steel
Found
70
Results
-- Page
1
2
of
2
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Instructions:
This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database. Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the
'Find'
button next to its box. You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.
Proto3000 - Rapid Prototyping
Notes:
Visit MatWeb's
property-based search page
to limit your results to materials that meet specific property performance criteria.
Text searches can be done from any page - use the
Quick Search
box in the top right of the page.
More
Search Strategies
on how to find information in MatWeb.
Show All Materials
- an inefficient drill-down to data sheets. Registered users who are logged in omit a step in this drill down process.
Top
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.