MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

AISI Grade 18Ni (200) Maraging Steel, Aged, 32 mm round bar, tested in longitudinal direction
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel; Maraging Steel

Material Notes: Applications: Bearings, Belleville springs, bolts, cannon recoil springs, rocket motor and missiles cases, couplings, load cells, flexures for guidance mechanisms of missiles, helicopter drive shafts, transmission shafts, fan shafts in commercial jet engines, aircraft wing components and forgings, aluminum die casting dies, cold forming dies, plastic molding dies, cores, pins, punches, and trim knees.

Key Words: maraging steels, UNS K92810, ASTM A538 (A), ASTM A579 grade 71
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 511511estimated, based on comparison with similar maraging steels.
Hardness, Knoop 567567estimated, based on comparison with similar maraging steels.
Hardness, Rockwell C 5252estimated, based on comparison with similar maraging steels.
Hardness, Vickers 546546estimated, based on comparison with similar maraging steels.
Tensile Strength, Ultimate 1844 MPa267500 psi
Tensile Strength, Yield 1780 MPa258000 psiestimated, based on comparison with similar maraging steels.
Elongation at Break 11 %11 %estimated, based on comparison with similar maraging steels.
Reduction of Area 57 %57 %estimated, based on comparison with similar maraging steels.
Modulus of Elasticity 183 GPa26500 ksi
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.300.30Calculated
Shear Modulus 70.0 GPa10200 ksiEstimated from elastic modulus
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000174 ohm-cm0.0000174 ohm-cmTypical steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.1 µm/m-°C
@Temperature 21.0 - 480 °C
5.61 µin/in-°F
@Temperature 69.8 - 896 °F
Thermal Conductivity  25.3 W/m-K
@Temperature 20.0 °C
176 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 25.8 W/m-K
@Temperature 50.0 °C
179 BTU-in/hr-ft²-°F
@Temperature 122 °F
 27.0 W/m-K
@Temperature 100 °C
187 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.10 %0.10 %
Boron, B 0.0030 %0.0030 %
Carbon, C <= 0.030 %<= 0.030 %
Cobalt, Co 8.5 %8.5 %
Iron, Fe 69 %69 %As remainder
Manganese, Mn <= 0.10 %<= 0.10 %
Molybdenum, Mo 3.25 %3.25 %
Nickel, Ni 18.5 %18.5 %
Phosphorus, P <= 0.010 %<= 0.010 %
Silicon, Si <= 0.10 %<= 0.10 %
Sulfur, S <= 0.010 %<= 0.010 %
Titanium, Ti 0.20 %0.20 %
Zirconium, Zr 0.010 %0.010 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Grade 18Ni (200) Maraging Steel, Annealed
AISI Grade 18Ni (250) Maraging Steel, Aged, 32 mm round bar, tested longitudinal
AISI Grade 18Ni (200) Maraging Steel, Aged, 16 mm round bar, tested in longitudinal direction
AISI Grade 18Ni (200) Maraging Steel, Aged, 75 mm round bar, tested in longitudinal direction
2800 Maraging Steel

M1820C / 7366

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.