MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Polypropylene with 60% Glass Fiber Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 60% Glass Fiber Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.15 - 2.10 g/cc0.0415 - 0.0759 lb/in³Average value: 1.47 g/cc Grade Count:36
Filler Content 60.0 %60.0 %Average value: 60.0 % Grade Count:5
Thickness 330 - 3320 microns13.0 - 131 milAverage value: 1650 microns Grade Count:6
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cm0.00100 - 0.00600 in/inAverage value: 0.00265 cm/cm Grade Count:7
 0.00100 - 0.00100 cm/cm
@Temperature 220 - 240 °C
0.00100 - 0.00100 in/in
@Temperature 428 - 464 °F
Average value: 0.00100 cm/cm Grade Count:4
 0.00100 - 0.00100 cm/cm
@Pressure 60.0 - 60.0 MPa
0.00100 - 0.00100 in/in
@Pressure 8700 - 8700 psi
Average value: 0.00100 cm/cm Grade Count:4
Linear Mold Shrinkage, Transverse 0.00100 - 0.00380 cm/cm0.00100 - 0.00380 in/inAverage value: 0.00227 cm/cm Grade Count:3
Melt Flow 4.00 - 10.0 g/10 min4.00 - 10.0 g/10 minAverage value: 6.33 g/10 min Grade Count:6
Ash 60.0 - 60.0 %
@Temperature 600 - 600 °C
60.0 - 60.0 %
@Temperature 1110 - 1110 °F
Average value: 60.0 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 41.9 - 931 MPa6070 - 135000 psiAverage value: 183 MPa Grade Count:28
 80.0 - 90.0 MPa
@Temperature 80.0 - 80.0 °C
11600 - 13100 psi
@Temperature 176 - 176 °F
Average value: 85.3 MPa Grade Count:4
Tensile Strength, Yield 16.5 - 150 MPa2400 - 21800 psiAverage value: 106 MPa Grade Count:14
Elongation at Break 1.00 - 3.40 %1.00 - 3.40 %Average value: 1.86 % Grade Count:29
 2.00 - 2.10 %
@Temperature 80.0 - 80.0 °C
2.00 - 2.10 %
@Temperature 176 - 176 °F
Average value: 2.03 % Grade Count:4
Elongation at Yield 1.40 - 8.00 %1.40 - 8.00 %Average value: 2.66 % Grade Count:8
Modulus of Elasticity 5.00 - 33.9 GPa725 - 4920 ksiAverage value: 14.6 GPa Grade Count:32
 9.10 - 9.50 GPa
@Temperature 80.0 - 80.0 °C
1320 - 1380 ksi
@Temperature 176 - 176 °F
Average value: 9.40 GPa Grade Count:4
Flexural Yield Strength 28.3 - 606 MPa4100 - 87900 psiAverage value: 227 MPa Grade Count:31
 134 - 141.343 MPa
@Temperature 80.0 - 80.0 °C
19400 - 20500.0 psi
@Temperature 176 - 176 °F
Average value: 138 MPa Grade Count:6
Flexural Modulus 0.145 - 33.2 GPa21.0 - 4820 ksiAverage value: 12.6 GPa Grade Count:40
 9.50 - 11.0316 GPa
@Temperature 80.0 - 80.0 °C
1380 - 1600.02 ksi
@Temperature 176 - 176 °F
Average value: 10.4 GPa Grade Count:6
Izod Impact, Notched 0.320 - 3.42 J/cm0.600 - 6.41 ft-lb/inAverage value: 2.36 J/cm Grade Count:7
Charpy Impact Unnotched 1.30 - 8.00 J/cm²6.19 - 38.1 ft-lb/in²Average value: 5.71 J/cm² Grade Count:20
 0.293 - 9.00 J/cm²
@Temperature -30.0 - -20.0 °C
1.39 - 42.8 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 5.58 J/cm² Grade Count:15
Charpy Impact, Notched 0.293 - 4.80 J/cm²1.39 - 22.8 ft-lb/in²Average value: 2.48 J/cm² Grade Count:26
 0.245 - 5.00 J/cm²
@Temperature -30.0 - -20.0 °C
1.17 - 23.8 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 2.69 J/cm² Grade Count:16
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.70 - 59.4 µm/m-°C5.39 - 33.0 µin/in-°FAverage value: 23.0 µm/m-°C Grade Count:4
 100.8 - 100.8 µm/m-°C
@Temperature 22.8 - 50.0 °C
56.00 - 56.00 µin/in-°F
@Temperature 73.0 - 122 °F
Average value: 101 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 14.0 - 64.6 µm/m-°C7.78 - 35.9 µin/in-°FAverage value: 31.2 µm/m-°C Grade Count:3
 66.6 - 66.6 µm/m-°C
@Temperature 22.8 - 50.0 °C
37.0 - 37.0 µin/in-°F
@Temperature 73.0 - 122 °F
Average value: 66.6 µm/m-°C Grade Count:1
Melting Point 160 - 173 °C320 - 343 °FAverage value: 166 °C Grade Count:20
Deflection Temperature at 0.46 MPa (66 psi) 124 - 164 °C255 - 327 °FAverage value: 154 °C Grade Count:10
Deflection Temperature at 1.8 MPa (264 psi) 85.0 - 175 °C185 - 347 °FAverage value: 152 °C Grade Count:29
Deflection Temperature at 8.0 MPa 138 - 140 °C280 - 284 °FAverage value: 139 °C Grade Count:4
Glass Transition Temp, Tg -10.0 - 165 °C14.0 - 329 °FAverage value: 48.3 °C Grade Count:3
Flammability, UL94 HBHBGrade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 30.0 - 270 °C86.0 - 518 °FAverage value: 176 °C Grade Count:13
Nozzle Temperature 204 - 270 °C400 - 518 °FAverage value: 241 °C Grade Count:7
Die Temperature 240 - 250 °C464 - 482 °FAverage value: 245 °C Grade Count:7
Melt Temperature 199 - 280 °C390 - 536 °FAverage value: 240 °C Grade Count:16
Mold Temperature 30.0 - 90.0 °C86.0 - 194 °FAverage value: 65.1 °C Grade Count:9
Drying Temperature 80.0 - 110 °C176 - 230 °FAverage value: 92.9 °C Grade Count:12
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.178 % Grade Count:8
Injection Pressure 40.0 - 140 MPa5800 - 20300 psiAverage value: 91.6 MPa Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 40% Glass Fiber Filler
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Overview of materials for Polypropylene, Molded

O4716 / 78381

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.