MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Master Builders Solutions ChemRex® 400 Construct Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: ChemRex 400 Construct Adhesive is a synthetic rubber-resin which bonds to concrete, masonry, metal, gypsum, cement board, asbestos cement board, and composition board. It can be applied with a caulking gun or power pump. Typical applications include gluing plywood subfloors to wood floor joints, adhering wallboard to studs, bonding paneling to furring strips, board to board laminations, and installation of ceramic tile.

Open time is 15 minutes ± 3 minutes depending on temperature and humidity. The percent solids is 65% ± 2% given the ASTM D 1259 test method. ChemRex 400 Construct Adhesive does not freeze. The lap shear is 410 psi on wet lumber, 570 psi on dry lumber, 480 psi on plywood/metal, and 270 on metal/metal. Each lap shear value is based on the ASTM D 3930 test method.

Information provided by ChemRex, Inc.

Product of former ChemRex, Inc. BASF launched the Master Builders Solutions brand on January 15, 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM D1475
Viscosity 250000 - 350000 cP250000 - 350000 cPASTM D2393
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 66.0 °C151 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREX01 / 65560

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.