MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum A383.0-F Die Casting Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A13830; Aluminium A383.0; AAA383.0; AlA383.0-F
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.68 g/cc0.0970 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8080
Tensile Strength, Ultimate 310 MPa45000 psi
Tensile Strength, Yield 152 MPa22000 psi
Elongation at Break 3.5 %3.5 %in 2"
Modulus of Elasticity 71.0 GPa10300 ksi
Fatigue Strength 131 MPa
@# of Cycles 5.00e+8
19000 psi
@# of Cycles 5.00e+8
Shear Strength 172 MPa25000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000750 ohm-cm0.00000750 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.7 µm/m-°C11.5 µin/in-°F
Thermal Conductivity 96.1 W/m-K667 BTU-in/hr-ft²-°F
Melting Point 516 - 571 °C960 - 1060 °F
Solidus 516 °C960 °F
Liquidus 571 °C1060 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 79.3 - 88.4 %79.3 - 88.4 %As remainder
Copper, Cu 2.0 - 3.0 %2.0 - 3.0 %
Iron, Fe <= 1.3 %<= 1.3 %
Magnesium, Mg 0.10 - 0.30 %0.10 - 0.30 %
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni <= 0.50 %<= 0.50 %
Other, total <= 0.50 %<= 0.50 %
Silicon, Si 9.5 - 11.5 %9.5 - 11.5 %
Tin, Sn <= 0.15 %<= 0.15 %
Zinc, Zn <= 3.0 %<= 3.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum A380.0-F Die Casting Alloy
Aluminum 384.0-F Die Casting Alloy
Aluminum 383.0-F Die Casting Alloy
Aluminum A383.1 Composition Spec
Aluminum A384.0-F Die Casting Alloy

MAC3830A / 10025

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.