MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum A384.0-F Die Casting Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium A384.0-F; UNS A13840; AAA384.0-F Die. 11.2Si-3.8Cu. Comparable to AC-46000 (AC46000) and AC-46100 (AC46100); AlA384.0-F
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.768 g/cc0.1000 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8585500 kg load, 10 mm ball
Hardness, Knoop 109109Estimated from Brinell Hardness.
Hardness, Rockwell A 3737Estimated from Brinell Hardness.
Hardness, Rockwell B 5353Estimated from Brinell Hardness.
Hardness, Vickers 9696Estimated from Brinell Hardness.
Tensile Strength, Ultimate 330 MPa47900 psi
Tensile Strength, Yield 165 MPa
@Strain 0.2 %
23900 psi
@Strain 0.2 %
Elongation at Break 2.5 %2.5 %in 50 mm
Machinability 50 %50 %0-100 Scale (100=best)
Shear Strength 198 MPa28700 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000750 ohm-cm0.00000750 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lbTypical for cast aluminum
CTE, linear  20.7 µm/m-°C
@Temperature 20.0 - 100 °C
11.5 µin/in-°F
@Temperature 68.0 - 212 °F
 22.1 µm/m-°C
@Temperature 20.0 - 300 °C
12.3 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°FTypical for cast aluminum
Thermal Conductivity 96.0 W/m-K666 BTU-in/hr-ft²-°F
Melting Point 516 - 582 °C961 - 1080 °F
Solidus 516 °C961 °F
Liquidus 582 °C1080 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 177 - 260 °C350 - 500 °FStress-relief anneal; hold at temperature 4 - 6 hrs; cool in still air
 260 - 371 °C500 - 700 °Ffor increased ductility; hold at temperature 4 - 6 hrs; furnace cool or cool in still air
Casting Temperature 616 - 699 °C1140 - 1290 °FDie Casting
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 79.3 - 86.5 %79.3 - 86.5 %As remainder
Copper, Cu 3.0 - 4.5 %3.0 - 4.5 %
Iron, Fe <= 1.3 %<= 1.3 %
Magnesium, Mg <= 0.10 %<= 0.10 %
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni <= 0.50 %<= 0.50 %
Other, total <= 0.50 %<= 0.50 %
Silicon, Si 10.5 - 12 %10.5 - 12 %
Tin, Sn <= 0.35 %<= 0.35 %
Zinc, Zn <= 1.0 %<= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum A380.0-F Die Casting Alloy
Aluminum 384.0-F Die Casting Alloy
Aluminum A383.0-F Die Casting Alloy
Aluminum A413.0-F Die Casting Alloy
Aluminum A360.0-F Die Casting Alloy

MAC3840AF / 10030

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.