MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AISI Type S14800 Stainless Steel condition C, 39.2% cold reduction
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless; T S10000 Series Stainless Steel

Material Notes: A precipitation-hardening stainless steel. Maintains high strength at elevated temperatures.

Key Words: UNS S14800, AMS 5601, AMS 5603; Precipitation Hardening
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 g/cc0.278 lb/in³In condition SRH950, 7.83 in condition A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 379379Converted from Rockwell C hardness.
Hardness, Knoop 414414Converted from Rockwell C hardness.
Hardness, Rockwell C 4141
Hardness, Vickers 396396Converted from Rockwell C hardness.
Tensile Strength, Ultimate 1227 MPa178000 psi
Tensile Strength, Yield 1034 MPa
@Strain 0.2 %
150000 psi
@Strain 0.2 %
Elongation at Break 8.0 %8.0 %in 50 mm
Modulus of Elasticity 200 GPa29000 ksiTypical for stainless steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.50 µm/m-°C
@Temperature 21.0 - 93.0 °C
5.28 µin/in-°F
@Temperature 69.8 - 199 °F
 10.6 µm/m-°C
@Temperature 21.0 - 205 °C
5.89 µin/in-°F
@Temperature 69.8 - 401 °F
 11.2 µm/m-°C
@Temperature 21.0 - 315 °C
6.22 µin/in-°F
@Temperature 69.8 - 599 °F
 11.5 µm/m-°C
@Temperature 21.0 - 540 °C
6.39 µin/in-°F
@Temperature 69.8 - 1000 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.75 - 1.5 %0.75 - 1.5 %
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 13.75 - 15 %13.75 - 15 %
Iron, Fe 73 %73 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 2.0 - 3.0 %2.0 - 3.0 %
Nickel, Ni 7.75 - 8.75 %7.75 - 8.75 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.010 %<= 0.010 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A228 Steel (UNS K08500)
AISI 6150H Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1060 Steel, oil quenched 845°C (1550°F), 480°C (900°F) temper, 25 mm (1 in.) round
AISI 1030 Steel, water quenched from 870°C (1600°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1006 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round

MQM14AS / 13498

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.