MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ZEON Hydrin® T3108 Epichlorohydrin Elastomer (ECO)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Hydrin T3108 is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with heat and oil resistance. Compounds using Hydrin T3108 typically exhibit excellent low- and high temperature properties and can be cured using conventional cure systems such as sulfur/sulfur donor or peroxides. Hydrin T3108 is supplied as bales sealed in an LDPE bag.

Hydrin® epichlorohydrin (ECO) elastomers provide an excellent balance of heat (125°C), oil, fuel, and ozone resistance with superior low temperature flexibility. Hydrin is broadly used in automotive fuel hose, air ducts, A/C, and vibration dampening. Its electrical properties benefit laser printer rolls. Hydrin is classified as a CH polymer according to SAE J200 / ASTM D2000.

Information provided by Zeon Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/cc
Mooney Viscosity 40 - 54
@Temperature 100 °C
40 - 54
@Temperature 212 °F
ML(1+4); MBL 1414/ASTM D-1646
Ash <= 1.0 %<= 1.0 %MBL 1358
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4242
Compression Set 5.8 %
@Temperature 70.0 °C,
Time 79200 sec
5.8 %
@Temperature 158 °F,
Time 22.0 hour
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 320000 ohm-cm320000 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Glass Transition Temp, Tg -48.0 °C-54.4 °F
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 18.1 - 20.1 %18.1 - 20.1 %MBL 1359
H2O, Water <= 1.0 %<= 1.0 %MBL 1361
 
Descriptive Properties
Age Content (%)6.2-8.2allyl glycidyl ether MBL 1357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZEON940 / 250119

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.