MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese FORTRON 1200L1 PPS, Specialty
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Fortron 1200L1 is an unfilled grade recommended primarily for extrusion applications. It has a high melt viscosity and tensile elongation. Recommended processing conditions are similar to those of our standard unfilled PPS grades.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Water Absorption at Saturation 0.020 %0.020 %ISO 62
Viscosity 430000 cP430000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9393ISO 2039-2
Tensile Strength at Break 88.0 MPa12800 psi50mm/min; ISO 527-2/1A
Elongation at Break 15 %15 %50mm/min; ISO 527-2/1A
Elongation at Yield 3.0 %3.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 4.00 GPa580 ksi50mm/min; ISO 527-2/1A
Flexural Strength 141 MPa20500 psiISO 178
Flexural Modulus 4.10 GPa595 ksiISO 178
Charpy Impact Unnotched 20.0 J/cm²95.2 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.0
@Frequency 10000 Hz
3.0
@Frequency 10000 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C22.2 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 42.0 µm/m-°C23.3 µin/in-°FISO 11359-2
Melting Point 275 °C527 °F10°C/min; ISO 11357-1,-2,-3
Glass Transition Temp, Tg 90.0 °C194 °FISO 11357-1,-2,-3
 
Processing PropertiesMetricEnglishComments
Drying Temperature 110 - 120 °C230 - 248 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
 
Descriptive Properties
Injection moldingYes
Sheet extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 317 PPS, Unfilled
Celanese FORTRON 1120L4 PPS, 20% Specialty
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced
Celanese FORTRON 1342L4 PPS, 40% Specialty
Celanese FORTRON 214 PPS, Unfilled

PHCQ275 / 178730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.