MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese FORTRON 1342L4 PPS, 40% Specialty
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Fortron 1342L4 is a low wear grade, ideally suited for bearings, gears and other sliding friction/wear applications. This product is glass fiber reinforced and contains PTFE.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccASTM D792
Density 1.69 g/cc0.0611 lb/in³ISO 1183
Water Absorption 0.020 %
@Temperature 22.8 °C
0.020 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Water Absorption at Saturation 0.020 %0.020 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4
 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 152 MPa22000 psiASTM D638
 165 MPa23900 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.6 %1.6 %5mm/min; ISO 527-2/1A
 2.0 %2.0 %ASTM D638
Tensile Modulus 14.4 GPa2090 ksi50mm/min; ISO 527-2/1A
Flexural Strength 231 MPa33500 psiASTM D790
 245 MPa35500 psiISO 178
Flexural Modulus 13.1 GPa1900 ksiASTM D790
 13.7 GPa1990 ksiISO 178
Izod Impact, Unnotched 0.854 J/cm1.60 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 8.50 kJ/m²
@Temperature -30.0 °C
4.04 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
Charpy Impact Unnotched 4.40 J/cm²20.9 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.850 J/cm²4.04 ft-lb/in²ISO 179/1eA
 0.850 J/cm²
@Temperature -30.0 °C
4.04 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Coefficient of Friction, Dynamic 0.160.16steel; ASTM D1894
 0.210.21Fortron; ASTM D1894
Coefficient of Friction, Static 0.200.20steel; ISO 8295
 0.200.20steel; ASTM D1894
 0.270.27Fortron; ASTM D1894
K (wear) Factor 334 x 10-8 mm³/N-M166 x 10-10 in³-min/ft-lb-hr416 Stainless,16 µ-in,90F,PV2000,40 psi,50 ft/min; ASTM D3702
 651 x 10-8 mm³/N-M323 x 10-10 in³-min/ft-lb-hrC-1018 steel,16 µ-in,120F,PV2000,40 psi,50 ft/min; ASTM D3702
 1660 x 10-8 mm³/N-M825 x 10-10 in³-min/ft-lb-hrC-1018 steel,16 µ-in,200F,PV2000,40 psi,50 ft/min; ASTM D3702
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C12.2 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 40.0 µm/m-°C22.2 µin/in-°FISO 11359-2
Melting Point 280 °C536 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 268 °C514 °FASTM D648
 270 °C518 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 215 °C419 °FISO 75-1, -2
Glass Transition Temp, Tg 90.0 °C194 °FISO 11357-1,-2,-3
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 140 - 160 °C284 - 320 °Fcavity
 330 - 340 °C626 - 644 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 290 - 300 °C554 - 572 °F
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 330 - 340 °C626 - 644 °F
Zone 4 330 - 340 °C626 - 644 °F
Die Temperature 310 - 330 °C590 - 626 °F
Melt Temperature 330 - 340 °C626 - 644 °F
Drying Temperature 130 - 140 °C266 - 284 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Injection Pressure 50.0 - 100 MPa7250 - 14500 psi
Hold Pressure 30.0 - 70.0 MPa4350 - 10200 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  50 rpm
@Diameter 55.0 mm
50 rpm
@Diameter 2.17 in
 75 rpm
@Diameter 40.0 mm
75 rpm
@Diameter 1.57 in
 120 rpm
@Diameter 25.0 mm
120 rpm
@Diameter 0.984 in
 
Descriptive Properties
Injection moldingYes
Injection speedfast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
Celanese FORTRON 4184L4 PPS, 53% Mineral / Glass Reinforced
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced
Celanese FORTRON 11400000000 PPS, 40% Glass Reinforced
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced

PHCQ276 / 178731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.