MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin HU1004 Polyetherimide (PEI) (Americas)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI); food contact compliant; Steam, Gamma, EtO, and E-beam sterilizable.

Features: Healthcare,Steam, Gamma, EtO and E-beam sterilizable,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,Steam Sterilizable,Gamma Sterilizable,E-beam Sterilizable,Food Contact Acceptable,Biocompatible

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/ccASTM D792
Density 1.28 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Viscosity 14 cP
@Load 5.00 kg,
Temperature 360 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPa50 mm/min; ISO 527
 90.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 95.0 MPa5 mm/min; ASTM D638
 97.0 MPa50 mm/min; ISO 527
Elongation at Break 80 %50 mm/min; ISO 527
 85 %5 mm/min; ASTM D638
Elongation at Yield 7.0 %5 mm/min; ASTM D638
 7.0 %50 mm/min; ISO 527
Tensile Modulus 2900 MPa5 mm/min; ASTM D638
Flexural Strength 136 MPayield, 2 mm/min; ISO 178
 140 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2800 MPa2 mm/min; ISO 178
 3000 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 70.0 JASTM D256
 3300 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact, Notched 11.0 kJ/m²ISO 179/2C
Dart Drop, Total Energy 93.0 JASTM D3763
 93.0 J
@Temperature -20.0 °C
ASTM D3763
 99.0 J
@Temperature 0.000 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=0.750 mm
UL 746A
 60 - 120 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=0.750 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 56.0 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 55.0 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
Thermal Conductivity 0.190 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 205 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 214 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 204 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 212 °CRate B/120; ISO 306
 212 °CRate B/50; ISO 306
 219 °CRate A/50; ISO 306
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.750 mm
UL 94
Smoke Density 0.70Flaming, Ds 4 min; ASTM E662
Oxygen Index 46 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 390 °C
Zone 2 335 - 390 °C
Zone 3 345 - 390 °C
Melt Temperature 355 - 390 °CInjection Molding
Mold Temperature 130 - 160 °C
Drying Temperature 150 °CInjection Molding
Dry Time 6.00 - 8.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
 
Descriptive Properties
Instrumented Dart Impact Ductility, 0°C100 %ASTM D3763
Instrumented Dart Impact Ductility, -20°C90 %ASTM D3763
Instrumented Dart Impact Ductility, 23°C100 %ASTM D3763

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82712 / 290659

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.