MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC ULTEM™ Resin HU1004 Polyetherimide (PEI) (Americas)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI); food contact compliant; Steam, Gamma, EtO, and E-beam sterilizable.

Features: Healthcare,Steam, Gamma, EtO and E-beam sterilizable,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,Steam Sterilizable,Gamma Sterilizable,E-beam Sterilizable,Food Contact Acceptable,Biocompatible

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/ccASTM D792
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 14 cP
@Load 5.00 kg,
Temperature 360 °C
14 cP
@Load 11.0 lb,
Temperature 680 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 10 g/10 min
@Load 6.60 kg,
Temperature 337 °C
10 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psi50 mm/min; ISO 527
 90.0 MPa13100 psi5 mm/min; ASTM D638
Tensile Strength, Yield 95.0 MPa13800 psi5 mm/min; ASTM D638
 97.0 MPa14100 psi50 mm/min; ISO 527
Elongation at Break 80 %80 %50 mm/min; ISO 527
 85 %85 %5 mm/min; ASTM D638
Elongation at Yield 7.0 %7.0 %5 mm/min; ASTM D638
 7.0 %7.0 %50 mm/min; ISO 527
Tensile Modulus 2.90 GPa421 ksi5 mm/min; ASTM D638
Flexural Strength 136 MPa19700 psiyield, 2 mm/min; ISO 178
 140 MPa20300 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.80 GPa406 ksi2 mm/min; ISO 178
 3.00 GPa435 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 70.0 J51.6 ft-lbASTM D256
 3300 J
@Thickness 3.20 mm
2430 ft-lb
@Thickness 0.126 in
reverse notched; ASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179/2C
Dart Drop, Total Energy 93.0 J68.6 ft-lbASTM D3763
 93.0 J
@Temperature -20.0 °C
68.6 ft-lb
@Temperature -4.00 °F
ASTM D3763
 99.0 J
@Temperature 0.000 °C
73.0 ft-lb
@Temperature 32.0 °F
ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 100 - 175 V100 - 175 VUL 746A
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=0.750 mm
30 - 60 sec
@Thickness >=0.0295 in
UL 746A
 60 - 120 sec
@Thickness >=1.50 mm
60 - 120 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=0.750 mm
60 - 120 arcs
@Thickness >=0.0295 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
 56.0 µm/m-°C
@Temperature -20.0 - 150 °C
31.1 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
CTE, linear, Transverse to Flow  50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
 55.0 µm/m-°C
@Temperature -20.0 - 150 °C
30.6 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 214 °C
@Thickness 6.40 mm
417 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 204 °C
@Thickness 6.40 mm
399 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 212 °C414 °FRate B/120; ISO 306
 212 °C414 °FRate B/50; ISO 306
 219 °C426 °FRate A/50; ISO 306
UL RTI, Electrical 105 °C221 °FUL 746B
UL RTI, Mechanical with Impact 105 °C221 °FUL 746B
UL RTI, Mechanical without Impact 105 °C221 °FUL 746B
Flammability, UL94 V-0
@Thickness >=0.750 mm
V-0
@Thickness >=0.0295 in
UL 94
Smoke Density 0.700.70Flaming, Ds 4 min; ASTM E662
Oxygen Index 46 %46 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 345 - 390 °C653 - 734 °F
Zone 2 335 - 390 °C635 - 734 °F
Zone 3 345 - 390 °C653 - 734 °F
Melt Temperature 355 - 390 °C671 - 734 °FInjection Molding
Mold Temperature 130 - 160 °C266 - 320 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourInjection Molding
 24.0 hour24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
Instrumented Dart Impact Ductility, 0°C100 %ASTM D3763
Instrumented Dart Impact Ductility, -20°C90 %ASTM D3763
Instrumented Dart Impact Ductility, 23°C100 %ASTM D3763

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82712 / 290659

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.