MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Armacell OleTex® CDJN200 Polyethylene/EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Polyethylene (PE)

Material Notes:

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 lb/ft³ASTM D3575W
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 46.0 psiASTM D3575T
Elongation at Break 220 %ASTM D3575T
Compressive Strength 2.10 psi
@Strain 10 %
ASTM D3575D
 4.80 psi
@Strain 25 %
ASTM D3575D
 8.80 psi
@Strain 40 %
ASTM D3575D
 12.8 psi
@Strain 50 %
ASTM D3575D
Tear Strength 13.0 pliASTM D3575G
Compression Set 22 %ASTM D3575B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °F
Minimum Service Temperature, Air -65.0 °F
 
Descriptive Properties
FlammabilityFMVSS302Pass at >1/4"
Thermal Stability<2%24 hrs @ 158°F, ASTM D3575S
Water Absorption<0.07 lb/sq ft(skived), ASTM D3575L

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Ateva® 2606A EVA polymer for adhesives, automotive, compounds and molding
Celanese Ateva® 9020 EVA polymer for photovoltaic
Arkema OREVAC® 9307 Y EVA Terpolymer
Arkema OREVAC® 9309 EVA Terpolymer
Celanese Ateva® 1241 EVA polymer for compounds, flexible packaging and foam

PARMD125 / 186736

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.