MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema OREVAC® 9307 Y EVA Terpolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as free flowing natural coloured granules. Applications include skin packaging adhesive and thermo-adhesive films.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³ASTM D1505
Vinyl Acetate Content 13 - 15 %13 - 15 %Arkema
Melt Index of Compound 9.5 - 11.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.5 - 11.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ASTM D2240
Tensile Strength at Break 19.0 MPa2760 psiASTM D638
 26.0 MPa3770 psiFilm Property, 50 µm thickness; ASTM D882
Tensile Strength, Yield 4.80 MPa696 psiASTM D638
 5.60 MPa812 psiFilm Property, 50 µm thickness; ASTM D882
Elongation at Break 600 - 900 %600 - 900 %ASTM D638
 700 - 900 %700 - 900 %Film Property, 50 µm thickness; ASTM D882
Dart Drop Test 180 g0.397 lbASTM D1709
 
Thermal PropertiesMetricEnglishComments
Melting Point 93.0 °C199 °FDSC
Vicat Softening Point 66.0 °C151 °FASTM D1525
Ring & Ball Softening Point 145 °C293 °F
 
Optical PropertiesMetricEnglishComments
Haze 3.5 %
@Thickness 0.0500 mm
3.5 %
@Thickness 0.00197 in
Film; ASTM D1003
 
Descriptive Properties
MAH Mini1600

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema OREVAC® 9309 EVA Terpolymer
Arkema Orevac® 18216 Maleic Anhydride modified EVA
Arkema OREVAC® 9304 EVA Terpolymer
Celanese Ateva® 2606A EVA polymer for adhesives, automotive, compounds and molding
Arkema Orevac® 9304 Film EVA-MAH Terpolymer

PARKG166 / 80127

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.