MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Domo TECHNYLSTAR® AF 218 V30 BLACK 21N PA 66 30% Glass Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYLSTAR® AF 218 V30 BLACK 21N is a polyamide 6.6, high flow, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in black color.

Key Properties: Easy processing; Heat stabilized; Suitable for Mucell®; Good surface aspect

Benefits: This product has enhanced molding behaviors and better surface aspect. It offers an excellent combination between thermal and mechanical properties. This grade is ideal for use in the automotive industry for engine components.

Applications: This grade is suitable for all kind of applications in automotive (pulleys, inlet manifolds, air ducts, engine covers...) and non automotive that required a good balanced behavior between surface aspect, thermal and mechanical behavior.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 4.2 %4.2 %ISO 527 Type 1A
Charpy Impact Unnotched 8.00 J/cm²38.1 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Domo TECHNYLSTAR® AF 219 V30 PA 66 30% Glass Reinforced, Dry
Domo TECHNYLSTAR® AF 218 V25 BLACK 21N PA 66 25% Glass Reinforced, Dry
Akro-Plastic Akroloy® PA GF 30 natural (3177) PA 66 + PA 6I/6T Dry, 30% Glass Filled

PSOLVAY870 / 218598

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.