MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaolite 2800 Cast Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Crystalline Silica. Cast installation. Kaolite 2800 Cast and 2800 Gun are general-purpose insulating monolithic for use at temperatures up to 2800°F (1538°C). They contain high-purity, calciumaluminate cements for improved strength and volume stability. This mix utilizes a high-purity calcium- aluminate cement that is specifically chosen for its casting characteristics. A gun version is available as well.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.538 - 1.731 g/cc
@Temperature 816 °C
fired
 1.698 - 1.858 g/cc
@Temperature 104 °C,
Time 86400 sec
dried
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00276 - 0.00552 GPadried 24 hours at 104°C
 0.00276 - 0.00552 GPafired 5 hours at 816°C
 0.00552 - 0.01034 GPafired 5 hours at temp use limit, °C
Compressive Strength 11.0 - 24.1 MPa
@Temperature 104 °C,
Time 86400 sec
Cold Crushing Strength, dried; ASTM C 133
 11.72 - 24.1 MPa
@Temperature 816 °C,
Time 18000 sec
Cold Crushing Strength, fired; ASTM C 133
 10.3 - 34.5 MPa
@Temperature 1538 °C,
Time 18000 sec
Cold Crushing Strength, fired; ASTM C 133
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.500 W/m-K
@Temperature 260 °C
ASTM C201
 0.550 W/m-K
@Temperature 538 °C
ASTM C201
 0.580 W/m-K
@Temperature 815 °C
ASTM C201
 0.620 W/m-K
@Temperature 1093 °C
ASTM C201
 0.690 W/m-K
@Temperature 1371 °C
ASTM C201
Maximum Service Temperature, Air <= 1538 °C
Shrinkage 0.00 - 0.20 %
@Treatment Temp. 104 °C,
Time 86400 sec
dried; ASTM C113
 0.10 - 1.0 %
@Treatment Temp. 1538 °C,
Time 18000 sec
fired; ASTM C113
 0.40 - 0.90 %
@Treatment Temp. 816 °C,
Time 18000 sec
fired; ASTM C113
 
Processing PropertiesOriginal ValueComments
Moisture Content 16 - 22 %casting by vibrating
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Al2O3 57 %
CaO 3.9 %
Fe2O3 0.70 %
K2O+Na2O 1.0 %Na2O & K2O
MgO 0.10 %
SiO2 36 %
TiO2 1.5 %
 
Descriptive Properties
Placement, average (kg)47

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6269 / 203053

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.