MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Melos Mecoline S TP 1030 F Halogen-free, thermoplastic, flame retardant sheathing
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, thermoplastic, flame retardant sheathing compound for low and medium voltage cables

Compound class: Sheathing

Compound category: TP

Flame retardant: ATH

Standards: DIN EN 50363-8 TM7; DIN VDE 0276-604 HM4; DIN VDE 0281 part 14 TM7; IEC 60092-360 SHF 1; VDE 0207 part 24 HM2, HM4; VDE 0250 part 215 HM5; UL 1277 Oil Res I; UL 1277 Oil Res II; IEC 60502-1 ST8

Typical applications: Halogen-free, low smoke, thermoplastic, highly oil and extra fuel resistant, flame retardant compound for the sheathing of low and medium voltage cables for moving applications. (e. g. Green Energy/Offshore)

Features: Flame retardant; Halogen-free; Low smoke; Flexible; Flexible at low temperatures; Oil resistant

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³pressed plaques, 155°C / 5 min; DIN EN ISO 1183-1A
pH >= 6.2>= 6.2Corrosivity; IEC 60754-2
Mooney Viscosity 62
@Temperature 160 °C
62
@Temperature 320 °F
ML (1+4); DIN ISO 289-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787pressed plaques, 155°C / 5 min; DIN ISO 7619-1
Tensile Strength 11.2 MPa1620 psiextruded tapes; IEC 60811-501
 6.80 MPa
@Temperature 100 °C,
Time 86400 sec
986 psi
@Temperature 212 °F,
Time 24.0 hour
extruded tapes, Diesel; IEC 60811-404
 9.80 MPa
@Temperature 150 °C,
Time 360000 sec
1420 psi
@Temperature 302 °F,
Time 100 hour
extruded tapes, Fluid IRM 902; IEC 60811-404
 9.895 MPa
@Temperature 136 °C,
Time 605000 sec
1435 psi
@Temperature 277 °F,
Time 168 hour
extruded tapes, After ageing in air oven; IEC 60811-501
 9.901 MPa
@Temperature 23.0 °C,
Time 86400 sec
1436 psi
@Temperature 73.4 °F,
Time 24.0 hour
extruded tapes, Diesel; IEC 60811-404
 10.002 MPa
@Temperature 70.0 °C,
Time 605000 sec
1450.7 psi
@Temperature 158 °F,
Time 168 hour
extruded tapes, Fluid IRM 903; IEC 60811-404
 10.304 MPa
@Temperature 80.0 °C,
Time 5.18e+6 sec
1494.5 psi
@Temperature 176 °F,
Time 1440 hour
extruded tapes, Fluid IRM 902; IEC 60811-404
 10.5952 MPa
@Temperature 100 °C,
Time 605000 sec
1536.71 psi
@Temperature 212 °F,
Time 168 hour
extruded tapes, Fluid IRM 902; IEC 60811-404
 10.95 MPa
@Temperature 70.0 °C,
Time 605000 sec
1588 psi
@Temperature 158 °F,
Time 168 hour
extruded tapes, Water purified; IEC 60811-404
Elongation at Break 305 %305 %extruded tapes; IEC 60811-501
 66 %
@Temperature -52.0 °C
66 %
@Temperature -61.6 °F
extruded tapes; DIN EN ISO 527
 260.47 %
@Temperature 100 °C,
Time 86400 sec
260.47 %
@Temperature 212 °F,
Time 24.0 hour
extruded tapes, Diesel; IEC 60811-404
 262 %
@Temperature 70.0 °C,
Time 605000 sec
262 %
@Temperature 158 °F,
Time 168 hour
extruded tapes, Fluid IRM 903; IEC 60811-404
 262.91 %
@Temperature 23.0 °C,
Time 86400 sec
262.91 %
@Temperature 73.4 °F,
Time 24.0 hour
extruded tapes, Diesel; IEC 60811-404
 287.92 %
@Temperature 80.0 °C,
Time 5.18e+6 sec
287.92 %
@Temperature 176 °F,
Time 1440 hour
extruded tapes, Fluid IRM 902; IEC 60811-404
 290.05 %
@Temperature 70.0 °C,
Time 605000 sec
290.05 %
@Temperature 158 °F,
Time 168 hour
extruded tapes, Water purified; IEC 60811-404
 295.85 %
@Temperature 100 °C,
Time 605000 sec
295.85 %
@Temperature 212 °F,
Time 168 hour
extruded tapes, Fluid IRM 902; IEC 60811-404
 298.9 %
@Temperature 136 °C,
Time 605000 sec
298.9 %
@Temperature 277 °F,
Time 168 hour
extruded tapes, After ageing in air oven; IEC 60811-501
 322.08 %
@Temperature 150 °C,
Time 360000 sec
322.08 %
@Temperature 302 °F,
Time 100 hour
extruded tapes, Fluid IRM 902; IEC 60811-404
Penetration  24
@Temperature 90.0 °C,
Time 21600 sec
24
@Temperature 194 °F,
Time 6.00 hour
[%] Hot pressure test, extruded tapes; IEC 60811-508
 24
@Temperature 100 °C,
Time 21600 sec
24
@Temperature 212 °F,
Time 6.00 hour
[%] Hot pressure test, extruded tapes; IEC 60811-508
 27
@Temperature 120 °C,
Time 21600 sec
27
@Temperature 248 °F,
Time 6.00 hour
[%] Hot pressure test, extruded tapes; IEC 60811-508
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Brittleness Temperature -70.0 °C-94.0 °FASTM D 746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 180 °C320 - 356 °FTool
 170 - 180 °C338 - 356 °FMaximum mass temperature
Zone 1 130 - 150 °C266 - 302 °F
Zone 2 140 - 160 °C284 - 320 °F
Zone 3 140 - 160 °C284 - 320 °F
Zone 4 150 - 170 °C302 - 338 °F
Zone 5 150 - 170 °C302 - 338 °F
Adapter Temperature 155 - 175 °C311 - 347 °F
Head Temperature 160 - 180 °C320 - 356 °F
Drying Temperature 60.0 - 70.0 °C140 - 158 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 38 %38 %pressed plaques, 165°C / 5 min.; ASTM D 2863 A
 
Descriptive Properties
Cold bend testNo cracksat -40°C, IEC 60811-504
Conductivity=0.6 µS/mmpressed plaques, 165°C / 5 min, IEC 60754-2
Main burning propertiesnot detectableHalogen content, IEC 754-1
Water absorption1.21 mg/cm2after 240h at 70°C, IEC 60811-402
 1.4 mg/cm2after 24h at 90°C, IEC 60811-402

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS010 / 296117

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.