MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior No. 315 No-Clean Soldering Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Eliminates the need for cleaning soldered boards.
  • May be conformal coated without post cleaning.
  • Can be used with lead free solder.
  • Conforms to ANSI-J-STD-004, Type ORL0.
Description: Superior No. 315 is specially formulated for wave soldering. This flux was designed for soldering high quality electronic printed circuit boards (PCBs), such as, through-hole, mixed technology, and surface mount assemblies while eliminating the need for a post cleaning operation. Superior No. 315 is formulated for foam and/or spray applications as supplied.

Applications: WAVE SOLDERING-Superior No. 315 No-Clean Flux may be applied by foam, spray, or wave application. The optimum topside PCB preheat temperature recommendation is 200-240ºF/93-115ºC. Too low a preheat setting is indicated by post-solder residues on PCBs that look like water stains.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.805 - 0.825 g/cc0.805 - 0.825 g/cc
Density 0.814 g/cc0.0294 lb/in³
Solids Content 1.8 - 2.2 %1.8 - 2.2 %
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 16 - 2216 - 22
 
Thermal PropertiesMetricEnglishComments
Flash Point 11.7 °C53.1 °FTCC Method
 
Processing PropertiesMetricEnglishComments
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
ColorWater white & clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSFLUX051 / 185735

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.