MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Clinton Aluminum Alumold® 1-500 Forged
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is suitable for polishing and texturing and is weldable. It is supplied in the forged, heat treated, quenched, cold compressed and aged condition. Alumold 1-500 Forged possesses better than normal mechanical properties in all sizes, excellent thermal conductivity and very good machinability together with good stability.

Applications:

  • Blow Molding
  • Injection Molding
  • RIM-Molding
  • Vacuum Forming
  • Foam Molding
  • Holders and Support Plates
  • Jig and Fixtures
  • Die Sets
  • Machine Frames
Technical Properties
  • High Thermal Conductivity - Reduction in cycle time, maintenance of consistent processing temperature and better plastic part dimensional control
  • Good Corrosion Resistance - Against most plastic materials
  • Machinability - Reduction of machine time lowers tooling costs and improves delivery time
  • Surface treatment - Can be anodized, hard chromed and nickel plated to increase wear and corrosion resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170170
Tensile Strength, Ultimate 483 MPa70000 psi18-20in thickness
 524 MPa76000 psi7-11in thickness
 524 MPa76000 psi11-15in thickness
 524 MPa76000 psi15-17in thickness
 534 MPa77400 psi6-7in thickness
Tensile Strength, Yield  414 MPa
@Strain 0.2 %
60000 psi
@Strain 0.2 %
18-20in thick
 463 MPa
@Strain 0.2 %
67100 psi
@Strain 0.2 %
11-15in thick
 463 MPa
@Strain 0.2 %
67100 psi
@Strain 0.2 %
15-17in thick
 463 MPa
@Strain 0.2 %
67100 psi
@Strain 0.2 %
7-11in thick
 473 MPa
@Strain 0.2 %
68600 psi
@Strain 0.2 %
6-7in thick
Elongation at Break 7.0 %7.0 %18-20in thickness
 9.0 %9.0 %7-11in thickness
 9.0 %9.0 %11-15in thickness
 9.0 %9.0 %15-17in thickness
 10 %10 %6-7in thickness
Modulus of Elasticity 71.7 GPa10400 ksi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 152.2 W/m-K1056 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
1201 Alloy forged rolled circle
Magnesium AZ80A-T6, Forged
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate
1460 Alloy, forged rolled circle
Alcoa QC-10® Aluminum Mold Alloy

NCLINT1 / 15871

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.