Platinised Carbon Ink is designed to be used for screen printing working electrodes. It has been optimized to give superior electrochemical performance and designed to be used for printing working electrodes. This ink is particularly suited for use with oxidase enzymes where hydrogen peroxide is generated and detected. Screen Printing Equipment: semi-automatic, manual Screen Types: stainless steel, polyester, mesh 156-230tpi Substrate: polyester, PVC, polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd. |