MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SunChemical Gwent C2000511D1 Platinized Carbon Ink
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Platinised Carbon Ink is designed to be used for screen printing working electrodes. It has been optimized to give superior electrochemical performance and designed to be used for printing working electrodes. This ink is particularly suited for use with oxidase enzymes where hydrogen peroxide is generated and detected.
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 156-230tpi
Substrate: polyester, PVC, polycarbonate or ceramic

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 40 - 43 %
@Temperature 130 °C
40 - 43 %
@Temperature 266 °F
Filler Content 2.7 %2.7 %Platinum
Viscosity 12000 - 18000 cP12000 - 18000 cP
Thickness 10.0 microns0.394 milCured, Printed through 230 stainless steel mesh with 13 micron emulsion
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 80.0 °C
0.167 hour
@Temperature 176 °F
 30.0 min
@Temperature 60.0 °C
0.500 hour
@Temperature 140 °F
Shelf Life 6.00 Month6.00 Month
 
Component Elements PropertiesMetricEnglishComments
Platinum, Pt 2.7 %2.7 %Theoretical
 
Descriptive Properties
Conductive Filler TypePlatinum
Coverage cm2/g850Using a 230 mesh stainless steel screen
Material TypeReady-To-Use Formulation
Solvent SystemEthoxy Propanol or Sericol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WGELZ9010 / 139323

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.