Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewable raw materials. ISO polymer designation: PA 10T/X. ASTM designation: PPA, polyphthalamide Grivory XE 4102 is an injection molding material. It has a low density and is electrically conducting The main distinguishing feature of Grivory HT, when compared to other polyamides, is its good performance at high temperatures. Parts made of Grivory HT provide high stiffness and heat distortion temperatures. Further attributes of Grivory HT are the low moisture absorption, good dimensional stability and excellent chemical resistance.Information provided by EMS Grivory |