Machinability and weldability are fair. Cold formability of these steels is good to excellent. This grade responds favorably to heat treating and cold work. |
UNS G10250, AMS 5075, AMS 5077, ASTM A29, ASTM A510, ASTM A512, ASTM A519, ASTM A575, ASTM A576, FED QQ-S-700 (G10250), MIL-S-11310 (CS1025), MIL-S-7952, MIL-S-7952A, MIL-T-3520, MIL-T-5066, SAE J403, SAE J412, SAE J414, DIN 1.1158, JIS S 25 C, JIS S 28 C |