MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AK Steel 410 Martensitic Stainless steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: AK Steel 410 provides good corrosion resistance plus high strength and hardness. It is magnetic in both annealed and hardened conditions. A wide range of properties can be developed with different heat treatments. Applications requiring moderate corrosion resistance and high mechanical properties are ideal for this alloy. Typical uses include flat springs, knives, kitchen utensils and hand tools.

Information provided by AK Steel

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.74 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 80
Tensile Strength, Ultimate 517 MPa
Tensile Strength, Yield 310 MPa
@Strain 0.2 %
Elongation at Break 25 %in 2 inches
Modulus of Elasticity 200 GPa
Fatigue Strength 186 MPa
@# of Cycles 1.00e+7 ,
Temperature 538 °C
 296 MPa
@# of Cycles 1.00e+7 ,
Temperature 454 °C
 400 MPa
@# of Cycles 1.00e+7 ,
Temperature 21.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000570 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.90 µm/m-°C
@Temperature 0.000 - 100 °C
 11.6 µm/m-°C
@Temperature <=649 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 24.9 W/m-K
@Temperature 100 °C
 28.7 W/m-K
@Temperature 500 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 11.5 - 13.5 %
Iron, Fe >= 84.28 %As Remainder
Manganese, Mn <= 1.0 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
410 Stainless Steel
AK Steel 420 Martensitic Stainless steel
440C Martensitic Stainless Steel (UNS S44004)
AK Steel 410 Cb Martensitic Stainless steel
AISI 440 Stainless Steel

NAKS102 / 14705

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.