MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NeoGraf GRAFOIL® GHH Standard Internal Combustion Laminate, Metal Reinforced
Categories: Carbon; Graphite

Material Notes: GRAFOIL® Grade GHH is a laminate made with GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, gasoline/diesel head gaskets, EGR valve sealing, and turbo charger gaskets. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced. Laminate Construction: GRAFOIL® Grade GTC ? micro-thin, phenolic-based adhesive ? 0.004" thick Low-Carbon Steel Grade 1008 or 1010 ? micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.12 g/cc0.0405 lb/in³Standard; Graphite
Thickness 610 microns24.0 milStandard; Laminate
 860 microns33.9 milStandard; Laminate
 1630 microns64.2 milStandard; Laminate
 
Mechanical PropertiesMetricEnglishComments
Compression Set 74 %
@Pressure 34.5 MPa
74 %
@Pressure 5000 psi
after 5000 psi load
 83 %
@Temperature 540 °C,
Time 18000 sec
83 %
@Temperature 1000 °F,
Time 5.00 hour
Air Aging
 
Descriptive Properties
Compressibility (%)36at 5000 psi load
 41Air Aging (5 hours at 540°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NeoGraf GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
Aremco Pyro-Paint™ 634-CA High Temperature Refractory Coating
CoorsTek CRB-100 Resin-Impregnated Carbon Graphite
CoorsTek CRB-500 Medium Strength Carbon Graphite
Graphite, Carbon, C

CGRAF937 / 107341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.