MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NeoGraf GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
Categories: Carbon; Graphite

Material Notes: GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typically 98% graphite. Grade GTB is the facing material for grades GHR, GHE, GHP, and GHW laminates. GTB is used in most standard industrial fluid sealing applications, including: chemical, petrochemical, refinery, and steam service. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced.

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.00 g/cc0.0361 lb/in³Standard for 0.020", 0.040" 0.060" thick
 1.12 g/cc0.0405 lb/in³Standard for 0.005", 0.010", 0.015", 0.020", 0.025", 0.030", 0.060" thick
Thickness 130 microns5.12 milStandard
 250 microns9.84 milStandard
 380 microns15.0 milStandard
 510 microns20.1 milStandard
 640 microns25.2 milStandard
 760 microns29.9 milStandard
 1020 microns40.2 milStandard
 1520 microns59.8 milStandard
Ash 1.8 %1.8 %
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Cl (Chloride) 10 ppm10 ppmLeachable
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 4.48 MPa650 psiTypical for 70 lb/ft³
Compression Set 85 %
@Pressure 34.5 MPa
85 %
@Pressure 5000 psi
Typical for 70 lb/ft³
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 525 °C977 °F
Minimum Service Temperature, Air -240 °C-400 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 98.2 %98.2 %
Sulfur, S 0.055 %0.055 %
 
Descriptive Properties
Compressibility (%)43at 5000 psi load; Typical for 70 lb/ft³

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NeoGraf GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material
NeoGraf eGRAF® SPREADERSHIELD™ SS400 Graphite
NeoGraf GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material
NeoGraf GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material
NeoGraf GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material

CGRAF929 / 107333

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.