MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Garlock 706 Compressed Inorganic Fiber Gasketing, Nitrile Binder
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Inorganic fibers with a nitrile binder.
  • Inorganic, asbestos-free fibers offer superior performance in saturated and superheated steam
  • Thermally stable fibers retain effective seal even during thermal cycling to 750°F (400°C)
  • Unique manufacturing process minimizes cold flow and creep relaxation problems
  • Ideal for standard ANSI flanged connectors, as well as turbine crossover piping connectors
  • Multiple applications in power generation, chemical processing, hydrocarbon processing, and other industries
Media: Steam, oils, grease, water, heat transfer fluids

Information provided by Garlock Rubber Technologies

Key Words: butadiene acrylonitrile
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 105 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1400 psiacross grain; ASTM F152
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 25.0 V/mil100% RH for 96 hours; ASTM D149
 133 V/mil
@Temperature 121 °C,
Time 10800 sec
0.0625 in. thickness; ASTM D149
 142 V/mil
@Temperature 121 °C,
Time 10800 sec
0.125 in. thickness; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1000 °F
 750 °F
@Pressure 10.3 MPa
Continuous
Minimum Service Temperature, Air -100 °F
 
Descriptive Properties
ColorWhite
Compressibility, %7-17ASTM F36
Creep Relaxation, %18ASTM F38
Sealability ASTM F37B, ml/hr0.5ASTM Fuel A
 4Nitrogen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Garlock 362 Nitrile Sheet Rubber
Garlock 361 Nitrile Sheet Rubber
Garlock 5360 Nitrile Sheet Rubber
Garlock 9122 Nitrile Sheet Rubber Gasketing

PGARL849 / 157503

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.