MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Adflex X 190 G Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adflex X 190 G is a reactor TPO (thermoplastic polyolefin) manufactured using the Lyondell Basell's proprietary Catalloy process technology. It has been developed as an impact modifier for polypropylene to be used both in extrusion and in injection molding applications. Thanks to its particular characteristics, it does not alter the transparency of the modified polypropylene (homopolymer or random copolymer). Adflex X 190 G exhibits a high softness and a low modulus, with a relatively high Melt Flow Index. It does not contain any slip nor anti-blocking agents. The grade is available in natural pellet form.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Crates; Hot Melt Adhesives; Housewares; Impact Modification; Industrial Packaging; Peelable Film; Sports, Leisure & Toys

Market: Consumer Products; Flexible Packaging

Processing Method: Compounding; Injection Molding

Attribute: Good Flexibility; Good Processability; Low Temperature Impact Resistance; Medium Flow; Soft

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccISO 1183-1
Melt Flow 8.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 30.0
@Time 15.0 sec
ISO 868
Tensile Strength at Break 12.0 MPaISO 527-1, -2
Elongation at Break 600 %ISO 527-1, -2
Flexural Modulus 80.0 MPaISO 178
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -40.0 °C
ISO 179
 NB
@Temperature 23.0 °C
ISO 179
 NB
@Temperature -20.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °CUnannealed; ISO 75B-1, -2
Vicat Softening Point 56.0 °CA/50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9010 / 323938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.