MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MarkeTech Yttrium aluminum perovskite:Cerium (YAP:Ce; YAlO3) Scintillator Crystal  (discontinued **)
Categories: Ceramic; Oxide

Material Notes: Yttrium aluminum perovskite activated by cerium is a fast, mechanically strong and chemically resistant scintillation material. Mechanical properties enable precise machining and entrance windows can be made with a very thin aluminum layer deposited directly on the entrance surface of the crystal. YAP:Ce scintillators have very low energy secondary X-ray emissions which makes them desirable for imagining applications. YAP:Ce detectors are used for gamma and X-ray counting, electron microscopy, electron and X-ray imaging screens, and tomography systems.

Data provided by MarkeTech International. MarkeTech International is no longer in business.

Key Words: YAlO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.37 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 8.6
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.00 - 11.0 µm/m-°C
Melting Point 1875 °C
 
Descriptive Properties
Crystal StructureRhombohedral
Hydroscopic?No
Luminescence: Afterglow<0.005%at 6 ms
Luminescence: Decay Constant25 n/s
Luminescence: Integrated Light Output40NaI:Tl = 100
Luminescence: Photon Yield10300K; 103 pH/MeV
Luminescence: Radiation Length2.7 cm
Luminescence: Wavelength of max emissions370 nm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SAES Getters Nd:YAG Solid State Laser Crystals (Nd-doped Y3Al5O12)
Yttrium Aluminum Oxide, Y3Al5O12
MarkeTech Yttrium aluminum garnet:Ce (YGA:Ce; Y3Al5O12) Scintillator Crystal
American Elements Lanthanum Oxide Nanopowder
American Elements Holmium Nanoparticles

C5MT838 / 120747

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.