MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SAES Getters Nd:YAG Solid State Laser Crystals (Nd-doped Y3Al5O12)  (discontinued **)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Y3-xNdxAl5O12 where Nd doping level between 0.2 and 1.4% atomic. Among solid-state laser crystals, Nd:YAG is the most versatile and suitable for a wide range of applications due to its physical properties, low threshold, high gain and narrow linewidth. Typical applications include the military, medicine and material processing industries for cutting, welding, drilling, marking and repairing. Nd:YAG lasers are also employed in application areas characterized by harsh environmental conditions, like remote sensing, ocean and atmospheric experiments. Ultrapure gas and superior raw material purity, together with a tightly controlled proprietary process, allow us to proudly offer premium grade Nd:YAG crystal rods with low losses and superior efficiency.

Nd concentration uniformity along each rod is achieved by using only a small portion (about 20%) of the melt. A very uniform Nd profile is certified for each boule, that is also marked with laser for identification.

Information provided by SAES Getters.

Key Words: Neodymium YAG (Yttrium Aluminum Garnet Y3Al5O12)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.55 g/cc0.164 lb/in³
a Lattice Constant 12.01 Å12.01 Å
Molecular Weight 595.3 g/mol595.3 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 8.58.5
 
Thermal PropertiesMetricEnglishComments
CTE, linear  7.70 µm/m-°C
@Temperature 110 °C
4.28 µin/in-°F
@Temperature 230 °F
 7.80 µm/m-°C
@Temperature 111 °C
4.33 µin/in-°F
@Temperature 232 °F
 8.20 µm/m-°C
@Temperature 100 °C
4.56 µin/in-°F
@Temperature 212 °F
Specific Heat Capacity 0.590 J/g-°C0.141 BTU/lb-°F
Thermal Conductivity 13.0 W/m-K90.2 BTU-in/hr-ft²-°F
Melting Point 1970 °C3580 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.817
@Wavelength 1064 nm
1.817
@Wavelength 1064 nm
1064 nm
 
Descriptive Properties
Crystal StructureCubic - Garnet
Lasing Wavelength1064 nm
Primary Diode Pump Band808.6 nm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Yttrium aluminum garnet:Ce (YGA:Ce; Y3Al5O12) Scintillator Crystal
Yttrium Aluminum Oxide, Y3Al5O12
MarkeTech Yttrium Vanadate (YVO4) Fiber Optic Crystal
Schott N-BK7 Glass
MarkeTech Beta Barium Borate (BBO) NLO Single Crystal

CSAES02 / 1961

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.